A processing technology, solid wood door technology, applied in wood processing equipment, wood treatment, impregnated wood, etc., can solve the problems of substandard drying, poor paint absorption, heavy weight, etc., to enhance corrosion resistance and durability, reduce degumming or Cracking, increased durability effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] The processing technology of a kind of durable and solid carved solid wood door provided by the present invention comprises the following steps: A. Peel and air-dry the log material, then place it in an acidic solution pool and soak it for 15 days, then take it out and put it into a drying oven Carry out preheating treatment to the log material, place the log material after the preheating treatment in vacuum drying equipment and carry out drying treatment for 10 days, adopt gradual heating during the drying treatment, the drying temperature is first set to 30 degrees Celsius, and the last 3 days Set the drying temperature to 90 degrees Celsius, and finally cool naturally; B, cut the log material after drying in A into block-shaped small boards of equal width, length, and thickness, and then place the small boards in a concentration of 5% chlorine. In the sodium chloride solution, soak for 1 day, then take it out and carry out drying treatment, the moisture content of the...
Embodiment 2
[0022] The processing technology of a durable and strong carved solid wood door provided by the present invention comprises the following steps: A. Peel and air-dry the log material, then place it in an acidic solution pool and soak it for 22 days, then take it out and put it into a drying oven Carry out preheating treatment to the log material, place the log material after the preheating treatment in the vacuum drying equipment and carry out drying treatment for 13 days, adopt gradual heating during the drying treatment, the drying temperature is first set to 40 degrees Celsius, and the last 4 days , set the drying temperature to 95 degrees centigrade, and finally cool naturally; B, cut the log material after the drying treatment in A into block-shaped small boards of equal width, length and thickness, and place the small boards in a concentration of 8% Soak in sodium chloride solution for 2 days, then take out and carry out drying treatment, the moisture content of described ...
Embodiment 3
[0025]The processing technology of a durable and solid carved solid wood door provided by the present invention comprises the following steps: A. Peel and air-dry the log material, then place it in an acidic solution pool and soak it for 30 days, then take it out and put it into a drying oven Carry out preheating treatment to the log material, place the log material after the preheating treatment in the vacuum drying equipment and carry out drying treatment for 15 days, adopt gradual heating during the drying treatment, the drying temperature is first set to 50 degrees Celsius, and the last 5 days , set the drying temperature to 100 degrees Celsius, and finally cool naturally; B, cut the log material after the drying treatment in A into block small boards of equal width, length and thickness, and then place the small boards in a concentration of 10% In the sodium chloride solution, soak for 3 days, then take out and carry out drying treatment, the moisture content of described ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com