[0046] As an embodiment of the present invention, the raw materials are composed of the following parts by weight: 55 parts of clinoptilolite, 10 parts of medical stone, 8 parts of high CEC clay mineral, 25 parts of aluminum sulfate, 20 parts of calcium sulfate, 5 parts of magnesium oxide, 15 parts of diatomite, 25 parts of modified bentonite, 10 parts of modified volcanic rock, and 10 parts of attapulgite.
[0047] As an embodiment of the present invention, the raw materials are composed of the following parts by weight: 60 parts of clinoptilolite, 5 parts of medical stone, 10 parts of high CEC clay mineral, 30 parts of aluminum sulfate, 15 parts of calcium sulfate, 10 parts of magnesium oxide, 15 parts of diatomite, 20 parts of modified bentonite, 15 parts of modified volcanic rock, and 8 parts of attapulgite.
[0048] As an embodiment of the present invention, the raw materials are composed of the following parts by weight: 50 parts of clinoptilolite, 8 parts of medical sto...
experiment example 1
[0079] Experimental Example 1: Small Test of Polluted Water
[0080] Select raw materials according to the following proportions by weight: 55 parts of clinoptilolite, 10 parts of medical stone, 8 parts of high CEC clay mineral, 25 parts of aluminum sulfate, 20 parts of calcium sulfate, 5 parts of magnesium oxide, and 15 parts of diatomite , 25 parts of modified bentonite, 10 parts of modified volcanic rock, and 10 parts of attapulgite.
[0081] The preparation method of described modified bentonite is as follows:
[0082] (1) Get bentonite and put it into a beaker, add dilute sulfuric acid solution, stir while adding, until stirring evenly;
[0083] (2) After stirring the solution obtained in step (1) for 30 minutes, let it stand for 2 hours;
[0084] (3) place the solution after standing in a low-speed centrifuge and carry out centrifugation under the condition of 5000r / min, and take out the remaining solid;
[0085] (4) washing the solid obtained in step (3) with distill...
experiment example 2
[0105] Experimental Example 2: Surface Water Treatment
[0106] Select raw materials according to the following proportions by weight: 60 parts of clinoptilolite, 5 parts of medical stone, 10 parts of high CEC clay mineral, 30 parts of aluminum sulfate, 15 parts of calcium sulfate, 10 parts of magnesium oxide, and 15 parts of diatomite , 20 parts of modified bentonite, 15 parts of modified volcanic rock, and 8 parts of attapulgite.
[0107] The subject of the experiment is a river in Xiong'an New District. The river channel has received domestic sewage for a long time, and the stock pollution is serious, and the problem of ammonia nitrogen pollution is prominent. The effective water storage capacity of the experimental object is about 1000m 3 , dosage 800ppm, a total of 8 tons of ammonia nitrogen remover; test results see Figure 2-4 .
[0108] image 3 with Figure 4 They are the change diagrams of the river course after adding ammonia nitrogen agent. Such as figure ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com