A technology of foaming agent and water content, applied in the direction of chemical instruments and methods, drilling compositions, etc., can solve the problems of unfavorable long-term mining, large gas lift investment, large damage, etc., achieve good foam stabilization effect, reduce surface The effect of small tension and film thickness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] A foaming agent with low foam moisture content, which is composed of the following components in percentage by weight: 35% dioctylmethylhydroxysulfopropyl betaine, 1% sodium perfluorooctanesulfonate, polyethylene glycol 6000 4% and water 60%.
[0020] The preparation method comprises the steps of: mixing 35% by weight of dioctylmethyl hydroxysulfopropyl betaine and 60% by weight of water in a reaction vessel with constant temperature stirring and mixing, and then adding 4% by weight of poly Ethylene glycol 6000 was reacted for 0.5 h; after adding 1% by weight sodium perfluorooctane sulfonate and continuing to stir for 15 min, a foaming agent with low foam moisture content was obtained.
Embodiment 2
[0022] A foaming agent with low foam moisture content, consisting of the following components in percentage by weight: 38% dioctylmethylsulfopropyl betaine, 0.3% sodium perfluorooctanesulfonate, polyethylene glycol 6000 2% and water 59.7%. The structural formula of dioctylmethylhydroxysulfopropyl betaine is as follows figure 1 shown.
[0023] A method for preparing a foaming agent with a low foam moisture content, comprising the steps of stirring 38% by weight of dioctylmethyl sulfopropyl betaine and 59.7% by weight of water in a reaction vessel at constant temperature Mix evenly, then add 2% by weight of polyethylene glycol 6000 to react for 2 hours; add 0.3% by weight of sodium perfluorooctane sulfonate and continue stirring for 40 minutes to obtain a foam discharge agent with low foam moisture content.
Embodiment 3
[0025] A foaming agent with low foam moisture content, consisting of the following components in percentage by weight: 40% dioctylmethylsulfopropyl betaine, 0.4% sodium perfluorooctanesulfonate, polyethylene glycol 6000 1% and water 58.6%.
[0026] A method for preparing a foaming agent with a low foam moisture content, comprising the steps of: 40% by weight of dioctylmethyl sulfopropyl betaine and 58.6% by weight of water in a reaction vessel at a constant temperature of 50°C Stir and mix well, then add 1% by weight polyethylene glycol 6000 and react for 1 hour; add 0.4% by weight sodium perfluorooctane sulfonate and continue stirring for 30 minutes to obtain a foam discharge agent with low foam moisture content.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com