A technology of high temperature resistance and drilling fluid, which is applied in chemical instruments and methods, earthwork drilling, and flushing of wellbore, etc. It can solve the problems of water loss, wall building and inhibition, high temperature dispersion of bentonite, and rheological control of drilling fluid. Difficulty and other issues
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0041] The raw materials for the preparation of the high temperature resistant drilling fluid provided by the present invention preferably further include a weighting agent for increasing the density of the drilling fluid. The present invention has no special requirements on the amount of the weighting agent, and those skilled in the art can add it according to the density requirement of the high temperature resistant drilling fluid. The drilling fluid density of the present invention has strong adaptability and can be increased to 1.5g / cm 3 The above can effectively deal with high geostress formations. In the present invention, the weighting agent is preferably barite, and the present invention has no special limitation on barite, and any barite conforming to GB / T 5005-2010 drilling fluid material specification is applicable to the present invention. For example, barite powder produced by Hubei Longhai Chemical Co., Ltd., Puyang Longze Chemical Construction General Factory, ...
Embodiment 1
[0052] Add 2 grams of attapulgite, 4 grams of inorganic tackifier (select sepiolite soil powder) and 0.1 gram of alkalinity regulator (select NaOH) to 100 mL of water, and leave it for 24 hours after high-speed shearing for 20 minutes to make the soil powder fully water disperse to obtain a base slurry, recorded as 2% attapulgite + 4% inorganic tackifier + 0.1% NaOH. Among them, the meaning of 2% is: add 2 grams of slurry mixing materials to 100 mL of water, and the percentages appearing in subsequent formulas all have the same meaning. Keep stirring the base slurry, and add 0.6% high temperature resistant polymer fluid loss reducer SO-1, 4% high temperature resistant sulfonated fluid loss reducer OCL-JA, 4% high temperature resistant anti-slump agent Soltex, 5% high temperature stable agent HCOOK, 0.5% oxygen scavenger Na 2 SO 3 After stirring evenly, the high temperature resistant drilling fluid can be obtained.
[0053] The formula is recorded as: 2% attapulgite + 4% ino...
Embodiment 2
[0055] The difference from Example 1 is that the formula is: 2% attapulgite+4% inorganic tackifier+0.1%NaOH+0.6%SO-1+4%OCL-JA+3%Soltex+5%HCOOK+0.5 %Na 2 SO 3 +110% Barite.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com