A marine garbage collection device
A garbage collection and marine technology, which is used in transportation and packaging, special purpose ships, and open water surface cleaning. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] A marine garbage collection device, such as Figure 1-8 As shown, it includes a device body 1, a garbage transfer mechanism 2, a garbage conveying mechanism 3 and a garbage storage mechanism 4;
[0040] Such as figure 1 , 3 As shown in and 5, the device body 1 includes a hull 101, a pod propeller 102, and a cab 103. Two V-shaped notches 104 are symmetrically reserved on the head of the hull 101, and the inside of the hull 101 A cavity 106 is reserved, and a garbage collection port 105 communicating with the cavity 106 is provided on the two V-shaped notches 104, and a garbage collection groove 107 is reserved in the middle of the cavity 106. The pod propeller 102 is fixedly installed on the tail bottom of the hull 101, the driver's cabin 103 is fixedly installed on the upper part of the hull 101, and the driver's cabin 103 is arranged adjacent to the head of the hull 101;
[0041] Such as image 3 and 5 As shown in -7, the garbage transfer mechanism 2 is installed ...
Embodiment 2
[0059] The difference from Example 1 is that the surface of the hull 101 is also provided with a protective layer, and the protective layer is prepared by the following method:
[0060] Take the following raw materials and weigh them by weight: 15-20 parts of epoxy resin, 6-10 parts of calcium carbonate powder, 6-10 parts of titanium dioxide powder, 8-10 parts of phenolic resin, 8-10 parts of ceramic microbeads, and 8 parts of acrylic emulsion -10 parts, 2-4 parts of alcohol ester dodecane, 2-4 parts of triethanolamine, 1-3 parts of emulsified silicone oil and 30-40 parts of water;
[0061] S1. Add the weighed acrylic emulsion, alcohol ester dodeca, triethanolamine, emulsified silicone oil and water into the mixer and stir for 20-30min at a stirring speed of 600-800r / min to prepare a mixed solution;
[0062] S2, adding epoxy resin, calcium carbonate powder, titanium dioxide powder, phenolic resin and ceramic microbeads into the pulverizer and pulverizing until the particle dia...
PUM