A technology for water-based colorful coatings and raw materials, applied in the field of coatings, can solve problems such as difficult construction, colored particles sticking into agglomerates, etc., and achieve the effects of good water resistance and water whitening resistance, stable coating film, and high practical application prospects.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0110] The second aspect of the present invention provides a method for preparing the water-based colorful paint, which includes the following steps: after mixing the base paint with sand and gravel, divide it into several parts, add color paste to color, add protective glue and mix Granulate and sieve to obtain colored granules; add the obtained colored granules into the continuous phase to obtain water-based colorful paint.
[0111] In a preferred embodiment, the mixture ratio of the base paint and sand is 1:(0.7-1.3) by weight.
[0112] In a more preferred embodiment, the mixture ratio of the base paint and gravel is 1:1 by weight.
[0113]The sand used in the present invention is not particularly limited, and various sands known to those skilled in the art can be used, such as Guangxi Baisha.
[0114] In a preferred embodiment, the sandstone has a mesh number of 80-100 mesh.
[0115] In a more preferred embodiment, the mesh number of the sand is 90 mesh.
[0116] In the...
Embodiment 1
[0122] Embodiment 1 of the present invention provides a water-based multi-color paint, including a protective glue, a base paint, and a continuous phase, and the weight ratio of the three is 9:31:10.
[0123] The protective glue includes the following raw materials in parts by weight: 50 parts of thickener, 948 parts of water, and 2 parts of preservative. The thickener is lithium magnesium silicate, which is BZ-03 of Xiamen Jinbaisheng; the preservative is a preservative BIT with a content of 20wt%; the preparation method of the protective glue is: add the thickener to water and stir After 30 minutes, add the remaining raw materials and mix for 10 minutes to obtain.
[0124] The base paint includes the following raw materials in parts by weight: 300 parts of pure acrylic emulsion, 4 parts of dispersant, 5 parts of defoamer, 155 parts of filler, 7 parts of cellulose ether, 70 parts of thickener, 443 parts of water, 16 parts Auxiliary. The pure acrylic emulsion in the base pai...
Embodiment 2
[0128] Embodiment 2 of the present invention provides a water-based multicolor paint, including a protective glue, a base paint, and a continuous phase, and the weight ratio of the three is 5:25:7.
[0129] The protective glue includes the following raw materials in parts by weight: 30 parts of thickener, 800 parts of water, and 1 part of preservative. The thickener is lithium magnesium silicate, BZ-03 of Xiamen Jinbaisheng; the preservative is the preservative BIT with a content of 20wt%;
[0130] The base paint includes the following raw materials in parts by weight: 200 parts of pure acrylic emulsion, 1 part of dispersant, 3 parts of defoamer, 140 parts of filler, 5 parts of cellulose ether, 60 parts of thickener, 300 parts of water, 10 parts Auxiliary. The pure acrylic emulsion in the base paint is purchased from Bardford Company, the model is RS-2788, and the viscosity at 25° C. is 50 to 400 cps (the average viscosity is 225 cps); the dispersant in the base paint is sodi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com