Manufacturing method of low-smoke, low-toxicity and antistatic hook-and-loop fastener
A manufacturing method and technology of hook and loop fasteners, applied in fasteners, coatings, polyurea/polyurethane coatings, etc., can solve the problems of safety threats to surrounding personnel, high smoke toxicity, strong odor, etc., to accelerate electrostatic dissipation, Improve flame retardant performance and reduce the effect of static electricity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A method for manufacturing a low-smoke, low-toxicity, antistatic adhesive tape, the specific steps are as follows:
[0024] Step 1, first put the nylon Velcro into the exhaust dyeing machine for cleaning to remove the oil and stains on the surface of the fiber;
[0025] Step 2, put the cleaned nylon hook and loop into the exhaust dyeing machine for dyeing with halogen-free and heavy metal-free dyes, the temperature during dyeing is 90°C, and the dyeing time is 2 hours;
[0026] Step 3, dehydrating the dyed nylon hook and loop for 3 minutes;
[0027] Step 4: impregnate the hook-and-loop fastener and the hair-surface fastener separately, and impregnate the fastener with a flame-retardant finishing agent for 2 hours at a temperature of 30°C. After the impregnation, dehydrate the fastener for 2 minutes. Dry at 100°C for 2 minutes and bake at 130°C for 1 minute;
[0028] Step 5, drying the nylon Velcro at 100°C for 3 minutes;
[0029] Step 6: Coat the Velcro with the anti...
Embodiment 2
[0038] A method for manufacturing a low-smoke, low-toxicity, antistatic adhesive tape, the specific steps are as follows:
[0039] Step 1, first put the nylon Velcro into the exhaust dyeing machine for cleaning to remove the oil and stains on the surface of the fiber;
[0040] Step 2: Put the cleaned nylon Velcro into the exhaust dyeing machine for dyeing with halogen-free and heavy metal-free dyes, the temperature during dyeing is 98°C, and the dyeing time is 3 hours;
[0041] Step 3, dehydrating the dyed nylon Velcro for 5 minutes;
[0042] Step 4: impregnate the hook surface Velcro and the fur surface Velcro respectively, and impregnate the Velcro with a flame-retardant finishing agent for 6 hours at a temperature of 55°C. After the impregnation, dehydrate the Velcro for 10 minutes. Dry at 120°C for 8 minutes, and bake at 180°C for 6 minutes;
[0043] Step 5, drying the nylon Velcro at 105°C for 5 minutes;
[0044] Step 6: Coat the Velcro with the antistatic and flame-re...
Embodiment 3
[0053] A method for manufacturing a low-smoke, low-toxicity, antistatic adhesive tape, the specific steps are as follows:
[0054] Step 1, first put the nylon Velcro into the exhaust dyeing machine for cleaning to remove the oil and stains on the surface of the fiber;
[0055] Step 2, put the cleaned nylon hook and loop into the exhaust dyeing machine for dyeing with halogen-free and heavy metal-free dyes, the temperature during dyeing is 95°C, and the dyeing time is 2.5 hours;
[0056] Step 3, dehydrating the dyed nylon hook and loop for 4 minutes;
[0057] Step 4: impregnate the hook surface Velcro and the fur surface Velcro respectively, and impregnate the Velcro with a flame-retardant finishing agent for 4 hours at a temperature of 33°C. After the impregnation, dehydrate the Velcro for 4 minutes. Dry at 110°C for 5 minutes, and bake at 150°C for 3 minutes;
[0058] Step 5, drying the nylon Velcro at 102°C for 4 minutes;
[0059] Step 6: Coat the Velcro with the antistat...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com