Novel shielding type coaxial radio frequency cable and preparation method thereof
A radio frequency cable, shielded technology, applied in the field of new shielded coaxial radio frequency cable and its preparation, can solve the problems of offset wear, low degree of bonding, cable damage, etc. junction performance, the effect of improving mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Such as figure 1 As shown, a new shielded coaxial radio frequency cable includes a protective sheath layer 1, a shielding layer 2, an adhesive layer 3 and an inner core conductor 4; the surface of the inner core conductor 4 is fixedly connected with The protective sheath layer 1; the contact surface between the protective sheath layer 1 and the adhesive layer 3 is provided with accommodating grooves 11; the accommodating grooves 11 are evenly distributed on the circumference of the inner core conductor 4 as the center of the circle. On the inner wall of the protective sheath layer 1, the accommodating groove 11 is filled with the shielding layer 2; the two sides of the accommodating groove 11 are embedded with buffer elastic particles 12; the buffer elastic particles 12 are along the The edges of the accommodating grooves 11 are uniformly distributed, and both ends of the accommodating grooves 11 are sealed by a sealing rubber layer 13 .
[0030] In order to further re...
Embodiment 2
[0043] Change the raw materials of protective sheath layer 1 into mass parts: 20 parts of polypropylene, 10 parts of EPDM rubber, 2 parts of anti-aging agent, 5 parts of castor oil, 3 parts of aluminum oxide and 8 parts of modified phenolic resin; The raw materials of knot layer 3 are changed to mass parts: 10 parts of ethylene-vinyl acetate copolymer, 10 parts of hydroxypropyl methylcellulose, 30 parts of polyamide resin and 15 parts of graphene polymer; the rest of the structure and formula are the same as in the embodiment 1.
Embodiment 3
[0045] Change the raw materials of the protective sheath layer 1 into parts by mass: 40 parts of polypropylene, 15 parts of EPDM rubber, 8 parts of anti-aging agent, 6 parts of castor oil, 5 parts of aluminum oxide and 10 parts of modified phenolic resin; The raw materials of knot layer 3 are changed to mass parts: 15 parts of ethylene-vinyl acetate copolymer, 15 parts of hydroxypropyl methylcellulose, 40 parts of polyamide resin and 20 parts of graphene polymer; the rest of the structure, formula and steps are the same Example 1.