Foaming method of high-efficiency grinding head
A high-efficiency, foaming agent technology, applied in the field of mechanical equipment, can solve the problems that the board surface lines cannot be removed, increase the difficulty of wastewater treatment, and require a high number of revolutions, so as to reduce the motor load and reduce the difficulty of subsequent fine polishing , the effect of slow speed
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] The invention provides a technical solution:
[0023] A foaming method for a high-efficiency grinding head, comprising corundum, water-based glue, water-based foaming agent and flour, the weight parts of the carborundum, water-based glue, water-based foaming agent and flour are respectively 57 parts by weight of carborundum and 40 parts by weight of water-based glue. parts by weight, 1.5 parts by weight of water-based foaming agent and 1.5 parts by weight of flour.
[0024] Include the following steps:
[0025] Step 1: Take an appropriate amount of emery and water-based glue and place them in a mixing tank, and stir and mix them at a stirring speed of 100r / min. The foaming agent and flour are divided into three equal parts respectively, and only one-third of the raw materials are added each time, and the raw materials are divided into three times, and after all the raw materials are put in, stir at a fixed speed for 15 minutes;
[0026] Step 2: Add the stirred raw mat...
Embodiment 2
[0031] The invention provides a technical solution:
[0032] A foaming method for a high-efficiency grinding head, comprising corundum, water-based glue, water-based foaming agent and flour, the weight parts of the carborundum, water-based glue, water-based foaming agent and flour are respectively 57 parts by weight of carborundum and 37 parts by weight of water-based glue. parts by weight, 1.3 parts by weight of water-based foaming agent and 1.5 parts by weight of flour.
[0033] Include the following steps:
[0034] Step 1: Take an appropriate amount of emery and water-based glue and place them in a mixing tank, and stir and mix them at a stirring speed of 100r / min. The foaming agent and flour are divided into three equal parts respectively, and only one-third of the raw materials are added each time, and the raw materials are divided into three times, and after all the raw materials are put in, stir at a fixed speed for 15 minutes;
[0035] Step 2: Add the stirred raw mat...
Embodiment 3
[0040] The invention provides a technical solution:
[0041] A foaming method for a high-efficiency grinding head, comprising corundum, water-based glue, water-based foaming agent and flour, the weight parts of the carborundum, water-based glue, water-based foaming agent and flour are respectively 62 parts by weight of carborundum and 43 parts by weight of water-based glue. parts by weight, 1.5 parts by weight of water-based foaming agent and 1.7 parts by weight of flour.
[0042] Include the following steps:
[0043] Step 1: Take an appropriate amount of emery and water-based glue and place them in a mixing bucket, and stir and mix them at a stirring speed of 120r / min. The foaming agent and the flour are divided into three equal parts, and only one-third of the raw materials are added each time, and the raw materials are divided into three times, and all the raw materials are stirred at a fixed speed for 20 minutes;
[0044] Step 2: Add the stirred raw materials into the sh...