Composite activated carbon desulphurization agent and its prepn. method
A technology of composite activated carbon and desulfurizer, applied in separation methods, chemical instruments and methods, separation of dispersed particles, etc., can solve problems such as high operating costs, secondary pollution, and easy moisture absorption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0068] The invention includes the following raw materials: lime and thiourea by-products.
[0069] Lime: the chemical symbol is CaO, the chemical composition is CaO content > 95%, and the physical state is 0.5-3mm white granular.
[0070] Thiourea by-product: The main component of thiourea by-product is calcium hydroxide Ca(OH) 2 , 68% content, 3.8% magnesium oxide content, 5% activated carbon content, and more than 23% moisture. The physical state is 80 mesh black powder.
[0071] The present invention prepares raw materials by the following weight percentages:
[0072] Lime: 40-80%;
[0073] Thiourea by-product: 20-60%.
[0074] production method:
[0075] Preparation of raw materials: prepare raw materials according to the above formula.
[0076] High-temperature and high-pressure firing: In an autoclave with a diameter of 1.2×5 meters, the by-products of lime and thiourea react in the autoclave for 30 to 90 minutes, then the temperature rises to 260 to 280°C and the ...
Embodiment 2
[0093] The invention includes the following raw materials: lime, thiourea by-product, acidified weathered coal.
[0094] Lime: the chemical symbol is CaO, the chemical composition is CaO content > 95%, and the physical state is 0.5-3mm white granular.
[0095] Thiourea by-product: The main component of thiourea by-product is calcium hydroxide Ca(OH) 2 , 68% content, 3.8% magnesium oxide content, 5% activated carbon content, and more than 23% moisture. The physical state is 80 mesh black powder.
[0096] Acidified weathered coal: The main component of acidified weathered coal is humic acid, which contains a variety of chemical bonds, and its physical state is 120 mesh black powder. Acidified weathered coal contains a variety of chemical bonds and has a strong adsorption capacity. The preparation method of acidified weathered coal: Add the existing product weathered coal into sulfuric acid with a weight of 20% of the weight of the weathered coal and a concentration of 60%, re...
Embodiment 3
[0122] The invention includes the following raw materials: lime, by-products of thiourea, and activated carbon.
[0123] Lime: the chemical symbol is CaO, the chemical composition is CaO content > 95%, and the physical state is 0.5-3mm white granular.
[0124] Thiourea by-product: The main component of thiourea by-product is calcium hydroxide Ca(OH) 2 , 68% content, 3.8% magnesium oxide content, 5% activated carbon content, and more than 23% moisture. The physical state is 80 mesh black powder.
[0125] Activated carbon: The chemical symbol of the activated carbon is C, the chemical composition is activated carbon c, and the physical state is 100 mesh black powder.
[0126] The present invention prepares raw materials by the following weight percentages:
[0127] Lime: 40-70%;
[0128] Thiourea by-product: 20-56%;
[0129] Activated carbon: 3-15%.
[0130] production method
[0131] Raw material preparation: Prepare raw materials according to the formula.
[0132] High...