Beaded glass and method of manufacture
A manufacturing method and glass bead technology, which are applied in the field of glass beads and their manufacture, can solve the problems of limited new types of raw materials, easy falling off of dyeing layers, monotonous decorative effect, etc., and achieve good decorative effect, enhanced decorative effect, colorful optics, etc. effect of effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] According to the weight ratio of 100:3:1.5, the glass bead blank, bonding material and pearl powder are equipped, wherein the glass bead blank is made of colored (that is, the pigment is fused in the glass material) glass bead blank, and the bonding material is made of nitro varnish (selected Qingzhu brand nitro decorative paint, produced by Guangzhou Zhujiang Chemical Group Co., Ltd.), the pearl powder is mica titanium pearl powder.
[0019] Clean and dry the glass bead blanks; then add the glass bead blanks and the bonding material into the stirring device, and stir so that the surface of the glass bead blanks is covered with a layer of bonding material; when the bonding material layer is not dry, put the Add the pearl powder into the mixing equipment and stir it so that a layer of pearl powder is evenly adhered to the bonding material layer; then take out the coated glass bead blank from the mixing equipment, cool down and dry to obtain glass beads. The beads include...
Embodiment 2
[0022] According to the weight ratio of 100:2:1, the glass bead blank, bonding material and pearl powder are equipped, wherein the glass bead blank is made of colored (that is, the pigment is fused in the glass material) glass bead blank, and the bonding material is made of acrylic varnish (model is Jichen 2K#, produced by Huantong Paint Industry Co., Ltd., Zengcheng City, Guangdong Province), the pearlescent powder is made of mica titanium pearlescent powder.
[0023] Clean the glass bead blank and dry it; then add the pearlescent powder and the bonding material into the stirring equipment, and stir to make the pearlescent powder and the bonding material mix evenly; then add the glass bead blank into the stirring equipment, and stir to make The glass bead blank is covered with a layer of coating formed by the mixture of pearl powder and bonding material; then the coated glass bead blank is taken out of the stirring equipment, cooled and dried to obtain glass beads, which inclu...
Embodiment 3
[0026] According to the weight ratio of 100:3:1:0.5, it is equipped with glass bead blanks, bonding materials, pearl powder and metal powder, among which the glass bead blanks are colorless and transparent glass bead blanks, and the bonding material is acrylic varnish (model is Jichen 2K #, produced by Huantong Paint Industry Co., Ltd., Zengcheng City, Guangdong Province), the pearlescent powder is bismuth oxychloride, and the metal powder is copper powder.
[0027] Clean and dry the glass bead blanks; then add the glass bead blanks and the bonding material into the stirring device, and stir so that the surface of the glass bead blanks is covered with a layer of bonding material; when the bonding material layer is not dry, put the The required pearl powder and metal powder are added to the stirring equipment and stirred so that the pearl powder and metal powder are evenly adhered to the bonding material layer; then the coated glass bead blanks are taken out of the stirring equi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com