Method for producing industrial silicon by using petroleum coke as reducing agent
A petroleum coke and reducing agent technology, applied in chemical instruments and methods, silicon compounds, inorganic chemistry, etc., can solve the problem of rising impurity content in the bottom of the furnace, and achieve the effects of less impurity content, simple furnace body structure, and fast reaction speed
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0022] The present invention uses petroleum coke as reducing agent to produce the concrete steps of industrial silicon as follows:
[0023] 1] Raw material preparation: choose SiO 2 Content ≥99%, Fe 2 o 3 Content≤0.04%, Al 2 o 3 Silica with a content of ≤0.04%, CaO content of ≤0.01%, crushed to a particle size of 50-150mm, as a silicon source; powdered petroleum coke with a fixed carbon content of ≥80%, a volatile content of ≥13%, and an ash content of ≤2% is used for reduction Mix well according to the weight ratio of silica:petroleum coke=2:1, add into the submerged arc furnace; the submerged arc furnace includes three graphite electrodes that are distributed in the shape of "product" and respectively connected to the three-phase power frequency power supply, graphite The electrode is a hollow electrode;
[0024] 2] Reduction reaction: heat to the furnace temperature of 2400-2600°C, hold the temperature for 2 hours; stop heating, and pound the furnace; reheat to the fur...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com