Method for producing cation modified polyurethane color stabilizer
A production method and polyurethane technology are applied in the field of reactive film-forming fixatives and preparations for textiles, which can solve the problems of ineffective dyeing, and achieve the effects of improving color fastness and soft hand feeling.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0037] 1. Polyurethane prepolymerization reaction
[0038] Add 150 grams of polyether (2000) (i.e. PPG2000) and 50 grams of polyether (600) (i.e. PEG600) into a dry reaction kettle and distill under reduced pressure at 100°C for 1 to 1.5 hours to remove trace amounts of polyether polyols. moisture. After vacuuming, cool down to 80°C, add 5 grams of DMPA, stir to dissolve evenly, add 27.5 grams of TDI dropwise with a separatory funnel, and keep the reaction temperature between 80 and 90°C.
[0039] 2. Modified chain extension reaction
[0040] Dissolve 8 grams of diethylenetriamine in 100 grams of methyl ethyl ketone in advance, and after standing for 1 hour, drop it into the above prepolymer at room temperature, react for 2 hours, add 35-40 grams of water, and raise the temperature to 53 ° C. After reacting for 30 minutes, 8.1 g of epichlorohydrin was added dropwise, and the temperature was raised to 70° C. for 3 hours to react.
[0041] 3. Blocking reaction
[0042] When ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com