Anti-seepage pet pads and manufacturing method thereof
A manufacturing method and pet pad technology, applied in chemical instruments and methods, animal houses, lamination devices, etc., can solve problems such as leakage of pet pads, and achieve the effects of saving production costs, low energy consumption, and high output
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] The selected non-woven fabric has a weight of 10g / m 2 , The weight of dust-free paper is 10g / m 2 , The weight of toilet paper is 6g / m 2 , The weight of the waterproof membrane is 1g / m 2 , First stack a layer of non-woven fabric, a layer of dust-free paper, and a layer of toilet paper as the surface layer 11, the polymer absorbent layer and toilet paper as the middle layer 12, and the absorbent film as the bottom layer 13 in order. The electric heating roller performs hot pressing, the temperature of the hot pressing is 50°C, and the speed of the hot pressing is 60 sheets / min. After hot pressing, spray glue or paste double-sided tape on the bottom surface of the bottom layer, then paste non-sticky paper, and finally cut it into finished products and packaging.
Embodiment 2
[0036] The selected non-woven fabric has a weight of 1000g / m 2 , The weight of dust-free paper is 100g / m 2 , The weight of toilet paper is 60g / m 2 , The weight of the waterproof membrane is 60g / m 2 , First stack a layer of non-woven fabric, a layer of dust-free paper, and a layer of toilet paper as the surface layer 11, the polymer absorbent layer and toilet paper as the middle layer 12, and the absorbent film as the bottom layer 13 in order. The electric heating roller performs hot pressing, the temperature of the hot pressing is 260°C, and the speed of the hot pressing is 500 sheets / min. After hot pressing, spray glue or paste double-sided tape on the bottom surface of the bottom layer, then paste non-sticky paper, and finally cut it into finished products and packaging.
Embodiment 3
[0038] The selected non-woven fabric has a weight of 500g / m 2 , The weight of dust-free paper is 50g / m 2 , The weight of toilet paper is 30g / m 2 , The weight of the waterproof membrane is 30g / m 2 , First stack a layer of non-woven fabric, a layer of dust-free paper, and a layer of toilet paper as the surface layer 11, the polymer absorbent layer and toilet paper as the middle layer 12, and the absorbent film as the bottom layer 13 in order. The electric heating roller performs hot pressing, the temperature of the hot pressing is 150°C, and the speed of the hot pressing is 260 sheets / min. After hot pressing, spray glue or paste double-sided tape on the bottom surface of the bottom layer, then paste non-sticky paper, and finally cut it into finished products and packaging.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Basis weight | aaaaa | aaaaa |