Method for producing glued adhesion thick plate for construction
A production method and technology for structure, applied in the field of plywood production technology, can solve the problems of complex process, difficulty in ensuring the quality of plywood, and high production cost, and achieve the effects of simple process, excellent physical and mechanical properties, and high bonding strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] Use eucalyptus or poplar rotary-cut veneer as the core board, use melamine glue to coat evenly, form the billet, first cold press at 1MPa for 3 hours, and then hot press at 115°C and 1.2MPa for 20 minutes to obtain a thickness of 20mm The obtained plywood is sanded, trimmed, and toothed and tenoned in the length direction; clothed with PU glue, and finger-jointed to form a basic unit of plywood; the basic unit of plywood is evenly coated with PU glue, and the amount of glue is 200g / m 2 , and then thickened by cold pressing at 1.0MPa for 200 minutes, and processed into products with a thickness of 10cm.
Embodiment 2
[0022] Use eucalyptus or poplar rotary-cut veneer as the core board, use phenolic glue to coat evenly, form a billet, first cold press at 1.2MPa for 3 hours, and then hot press at 125°C and 1.5MPa for 30 minutes to obtain a plywood with a thickness of 25mm ; Sanding and trimming the obtained plywood, opening teeth and tenons in the length direction; clothing sbs resin glue, and finger jointing to form the basic unit of plywood; coating the basic unit of plywood with sbs resin glue evenly, and the amount of glue is 200g / m 2 , and then thickened by cold pressing at 1.9MPa for 320 minutes, and processed into a product with a thickness of 50cm.
Embodiment 3
[0024] Use eucalyptus or poplar rotary-cut veneer as the core board, use phenolic glue to coat evenly, form a billet, first cold press at 0.7MPa for 4 hours, and then hot press at 130°C and 1.0MPa for 25 minutes to obtain a 25mm thick plywood ; Sanding and trimming the obtained plywood, opening teeth and tenons in the length direction; clothing sbs resin glue, and finger jointing to form the basic unit of plywood; coating the basic unit of plywood with sbs resin glue evenly, and the amount of glue is 200g / m 2 , and then thickened by cold pressing at 1.2MPa for 240 minutes, and processed into products with a thickness of 30cm.