Embodiment 1
[0026] Weigh 4 g of sodium hypophosphite, 3 g of ammonium persulfate, 100 g of acrylic acid monomer, and 90 g of distilled water. Sodium hypophosphite and ammonium persulfate were respectively prepared with distilled water to form a sodium hypophosphite solution with a mass percent concentration of 30% and an ammonium persulfate solution with a mass percent concentration of 30%. Take 1 / 3 of the total volume of the ammonium persulfate solution and 1 / 4 of the total volume of the acrylic acid monomer, and drop them into the sodium hypophosphite solution at the same time, and then add the remaining distilled water. Heat to 65°C, adjust to keep warm, then continue to drop the remaining ammonium persulfate solution and acrylic acid monomer into the above reaction solution at the same time, and finish dropping within 1 hour. After dropping, keep warm at 65°C for 3 hours. Then, it was cooled to room temperature, and neutralized with 40% NaOH by mass percentage to make the pH of the s...
Embodiment 2
[0028] Same method as above. Sodium hypophosphite 4g, ammonium persulfate 10g, acrylic acid monomer 100g, distilled water 100g. Sodium hypophosphite and ammonium persulfate were prepared with distilled water to prepare sodium hypophosphite solution with a mass percent concentration of 25% and ammonium persulfate solution with a mass percent concentration of 25%. Take 1 / 4 of the total volume of the ammonium persulfate solution and 1 / 3 of the total volume of the acrylic acid monomer, and drop them into the sodium hypophosphite solution at the same time, and then add the remaining distilled water. Heat to 70°C, adjust to keep warm, then continue to drop the remaining ammonium sulfate solution and acrylic acid monomer into the above reaction solution, and finish dropping within 1 hour. After dropping, keep warm at 70°C for 3.5 hours. Then, it was cooled to room temperature, and neutralized with 40% NaOH by mass percentage to make the pH of the solution reach 8. Now the product ...
Embodiment 3
[0030] Same method as above, sodium hypophosphite 2g, ammonium persulfate 4g, acrylic acid monomer 100g, distilled water 100g. Sodium hypophosphite and ammonium persulfate were respectively prepared with distilled water to form a sodium hypophosphite solution with a mass percent concentration of 20% and an ammonium persulfate solution with a mass percent concentration of 20%. Take 1 / 4 of the total volume of the ammonium persulfate solution and 1 / 4 of the total volume of the acrylic acid monomer, and add them dropwise to the sodium hypophosphite solution at the same time, and then add the remaining distilled water. Heat to 65°C, adjust to keep warm, then continue to drop the remaining ammonium persulfate solution and acrylic acid monomer into the above reaction solution at the same time, and finish dropping within 1 hour. After dropping, keep warm at 70°C for 3 hours. Then, it was cooled to room temperature, and neutralized with 40% NaOH by mass percentage to make the pH of th...