Method for preparing aqueous ink special for cartons
A water-based ink and carton technology, which is used in the preparation of new printing inks, can solve the problems of small application range, high production cost and high price, achieve scientific simplicity, refine process conditions, and improve anti-corrosion and antibacterial properties, quality and performance. improved effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] 1. Preparation of rosin oil: the equipment adopts a 300Kg reactor.
[0014] (1) Add 150Kg of water and start heating;
[0015] (2) The water temperature rises to 65°C and 3Kg of methanol is added, then the stirrer is turned on and 75Kg of rosin resin is slowly added;
[0016] (3) The water temperature rises to 75°C-80°C and stirs for another 30 minutes, then adds 9Kg of monoethanolamine and continues to stir;
[0017] (4) When the water temperature drops below 70°C, add 1.5Kg of methanol and 9Kg of ammonia water and continue to stir for 2.5-3 hours until the pH value reaches 8.5-9.
[0018] 2. Grinding color paste:
[0019] Rosin oil 60Kg, carbon black 20Kg, water-based ink emulsified oil 7-9Kg, KE-309 paint ink defoamer 0.5Kg, water 100-200Kg, mix and grind until the fineness is below 15μm, it is the prepared color paste.
[0020] 3. Mixing ink:
[0021] Add 80-100Kg of rosin oil, 6Kg of water-based ink emulsified oil, 0.4Kg of KE-309 paint ink defoamer, 1Kg of mon...
Embodiment 2
[0027] 1. Preparation of rosin oil: the equipment adopts a 400Kg reactor.
[0028] (1) Add 200Kg of water and start heating;
[0029] (2) The water temperature rises to 65°C and 4Kg of methanol is added, then the stirrer is turned on and 100Kg of rosin resin is slowly added;
[0030] (3) The water temperature rises to 75°C-80°C and stirs for another 30 minutes, then adds 12Kg of monoethanolamine and continues to stir;
[0031] (4) When the water temperature drops below 70°C, add 2Kg of methanol and 12Kg of ammonia water and continue stirring for 2.5-3 hours until the pH value reaches 8.5-9.
[0032] 2. Grinding color paste:
[0033] Rosin oil 90Kg, carbon black 30Kg, water-based ink emulsified oil 8-9Kg, KE-309 paint ink defoamer 0.9Kg, water 150-200Kg, mix and grind until the fineness reaches below 15μm, it is the prepared color paste.
[0034] 3. Mixing ink:
[0035] Add 120-150Kg of rosin oil, 9Kg of water-based ink emulsified oil, 0.6Kg of KE-309 paint ink defoamer, 1....
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com