A technology of offset printing ink and water-based ink, which is applied in the direction of printing, printing machines, general parts of printing machinery, etc., can solve the problems of poor printing adaptability, storage stability, and long drying time, so as to promote the drying of offset printing ink and shorten production Cycle, reduce the effect of storage to dry time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] Prepare the water-based ink drier according to the following components in weight percent:
[0033] Aqueous Cobalt Drier 20%
[0034] Aqueous Manganese Drier 9%
[0035] Aqueous Calcium Drier 71%
[0036] Prepare the paper surface sizing solution according to the following components in weight percent:
[0037] Polyvinyl alcohol 5%
[0038] Melamine 1.2%
[0039] Urea 2.5%
[0040] Sodium Carboxymethyl Cellulose 0.5%
[0041] Water 90.8%
[0042] Then, the above-mentioned prepared water-based ink drier and paper surface sizing solution are operated as follows:
[0043] a. Prepare the paper surface sizing solution and water-based ink drier according to the following weight percentages
[0044] Paper surface sizing solution 93%
[0045] Water-based ink drier 7%
[0046] b. Attach the liquid prepared in step a to the surface of the paper by sizing;
[0047] c. drying the paper treated in step b, and dehydrating the water-based ink drier into an oil-based ink dri...
Embodiment 2
[0050] Prepare the water-based ink drier according to the following components in weight percent:
[0051] Aqueous Cobalt Drier 25%
[0052] Aqueous Barium Drier 75%
[0053] Prepare the paper surface sizing solution according to the following components in weight percent:
[0054] Polyvinyl alcohol 5%
[0055] Melamine 1.2%
[0056] Urea 2.8%
[0057] Water 91%
[0058] Then, the above-mentioned prepared water-based ink drier and paper surface sizing solution are operated as follows:
[0059] a. Prepare the paper surface sizing solution and water-based ink drier according to the following weight percentages
[0060] Paper surface sizing solution 95%
[0061] Water-based ink drier 5%
[0062] b. Attach the liquid prepared in step a to the surface of the paper by sizing;
[0063] c. drying the paper treated in step b, and dehydrating the water-based ink drier into an oil-based ink drier;
[0064] d. Print with offset printing ink on paper, the oily ink drier will play...
Embodiment 3
[0066] Prepare the water-based ink drier according to the following components in weight percent:
[0067] Aqueous Manganese Drier 40%
[0068] Aqueous Calcium Drier 60%
[0069] Prepare the paper surface sizing solution according to the following components in weight percent:
[0071] Melamine 1.2%
[0072] Urea 2.8%
[0073] Water 89%
[0074] Then, the above-mentioned prepared water-based ink drier and paper surface sizing solution are operated as follows:
[0075] a. Prepare the paper surface sizing solution and water-based ink drier according to the following weight percentages
[0076] Paper surface sizing solution 94%
[0077] Water-based ink drier 6%
[0078] b. Attach the liquid prepared in step a to the surface of the paper by sizing;
[0079] c. drying the paper treated in step b, and dehydrating the water-based ink drier into an oil-based ink drier;
[0080] d. Use offset printing ink to print on the paper, and the oil-based i...
PUM