Embodiment 1
[0051] (1) Preparation of protective colloid solution: Mix 94g of deionized water and 0.05g of sodium pyrophosphate and stir to dissolve evenly, then slowly add 5.95g of colloidal magnesium lithium silicate, and disperse at a high speed of 1200r / min for about 20min until complete dissolve, spare;
[0052] (2) Preparation of white base paint: 45g of deionized water, 0.2g of hydroxyethyl cellulose, 0.2g of dispersant, 0.2g of wetting agent, 0.1g of pH regulator, 0.05g of anti-mold and fungicide, defoamer Add 0.3g, 0.5g of film-forming aid, 1.5g of titanium dioxide, and 1.5g of calcined kaolin into the dispersion tank in sequence, disperse at high speed for 20min at a speed of 1200r / min, until the fineness reaches 20-30μm, and then add 40g of acrylic emulsion , stirring at a rotating speed of 400r / min for 5min, finally adding 10g of the protective colloid solution prepared in step (1), stirring evenly for subsequent use;
[0053] (3) Toning: according to the design requirements,...
Embodiment 2
[0057] (1) Preparation of protective colloid solution: Mix 93g of deionized water and 0.03g of sodium pyrophosphate and stir to dissolve evenly, then slowly add 5g of colloidal magnesium lithium silicate, and disperse at a high speed of 800r / min for about 30min until completely dissolved ,spare;
[0058] (2) Preparation of white base paint: 35g of deionized water, 0.1g of hydroxyethyl cellulose, 0.1g of dispersant, 0.1g of wetting agent, 0.05g of pH regulator, 0.01g of anti-mold and fungicide, defoamer Add 0.2g, 0.4g of film-forming aid, 2g of titanium dioxide, and 2g of calcined kaolin into the dispersing tank in sequence, disperse at high speed for 30min at a speed of 800r / min, until the fineness reaches 20-30μm, then add 30g of acrylic emulsion, Stir at 200r / min for 10min, finally add 7g of the protective colloid solution prepared in step (1), stir well and set aside;
[0059] (3) Toning: according to the design requirements, the white base paint prepared in step (2) is mi...
Embodiment 3
[0063] (1) Preparation of protective colloid solution: Mix 95g of deionized water and 0.06g of sodium pyrophosphate and stir to dissolve evenly, then slowly add 6g of colloidal magnesium silicate lithium, and disperse at a high speed of 1000r / min for about 20min until completely dissolved ,spare;
[0064] (2) Preparation of white base paint: 40g of deionized water, 0.3g of hydroxyethyl cellulose, 0.3g of dispersant, 0.2g of wetting agent, 0.1g of pH regulator, 0.05g of anti-mold and fungicide, defoamer Add 0.5g, 0.7g of film-forming aids, 2g of titanium dioxide, and 2g of calcined kaolin into the dispersion tank in sequence, disperse at high speed for 20min at a speed of 1000r / min, until the fineness is within the range of 20-30μm, and then add 35g of acrylic emulsion , stirring at a rotating speed of 300r / min for 10min, finally adding 9g of the protective colloid solution prepared in step (1), stirring evenly for later use;
[0065] (3) Toning: according to the design requir...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com