A technology for printing circuit boards and etching waste liquid, which is applied in chemical instruments and methods, multi-stage treatment of water/sewage, water pollutants, etc., can solve the problems of poor arsenic removal effect, high cost, secondary pollution, etc. To achieve the effect of easy control, low cost and small equipment investment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0041] A method for removing arsenic from printed circuit board alkaline etching waste liquid, comprising the steps of:
[0042] A 00 , sampling analysis and detection: get 500 milliliters of alkaline etching waste liquid of printed circuit board to be processed, to this waste liquid of alkaline etching of printed circuit board to be processed, sampling is analyzed and detected, and its arsenic content is 10ppm, namely 10 mg / L;
[0043] A 0 Pre-treatment: Pour 500 ml of the printed circuit board alkaline etching waste liquid into the reaction kettle, heat it to 80-90°C, then add 0.35 g of nano-scale activated carbon, and let it stand for 3 hours to absorb the alkaline Organic foam and impurities in the etching solution;
[0044] A. Magnesium chloride precipitation:
[0045] 1. weigh, take by weighing the magnesium chloride of 0.6 gram;
[0046] ② configure magnesium chloride solution, dilute the weighed magnesium chloride with water, such as adding 0.6 g of magnesium chlo...
Embodiment 2
[0055] A method for removing arsenic from printed circuit board alkaline etching waste liquid, comprising the steps of:
[0056] A 00 , sampling analysis and detection: the printed circuit board alkaline etching waste liquid to be treated is sampled for analysis and detection, and its arsenic content is 8ppm, i.e. 8 mg / liter;
[0057] A 0Pre-treatment: pump 60 cubic meters of alkaline etching waste liquid of printed circuit board into the treatment pool, heat it to 80-90°C, then add 30 kg of activated carbon to the nano-scale activated carbon, and let it stand for 5 hours to absorb organic foam and impurities in the alkaline etching solution;
[0058] A. Magnesium chloride precipitation:
[0059] 1. weigh, take by weighing 60 kilograms of magnesium chloride;
[0060] 2. configure magnesium chloride solution, dilute the weighed magnesium chloride with water, such as adding 60 kg of magnesium chloride to 1000 liters of water, stir to make it completely dissolved;
[0061] ③...