Beneficiation method for improving grade of manganese in rhodochrosite ores
A beneficiation method and rhodochrosite technology, applied in chemical instruments and methods, wet separation, solid separation, etc., can solve the problem of small embedded particle size, difficulty in enriching useful components in ore, and insufficient increase in the grade of rhodochrosite concentrate. major issues
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] Example 1: Rhodochrosite is taken from a mine in Laibin, Guangxi, and its composition characteristics are shown in Table 1.
[0013] Table 1 Chemical composition of rhodochrosite (%)
[0014] Element
[0015] Take 5Kg of rhodochrosite raw ore, after crushing and screening to obtain ore powder with a particle size of less than 25mm, carry out microwave roasting at a roasting temperature of 750°C and a roasting time of 25 minutes; after the roasting is completed, add water to the ore powder, and wet grind until the particle size is less than 1mm , the solid mass concentration in the grinding process is 70%, and the spiral chute is used to sort the grinding pulp to obtain manganese concentrate, and the additional water and pulp during sorting are fed into the spiral chute at the same time, and the solid mass concentration in the sorting process is The manganese grade in manganese concentrate is 21.5%, and the manganese recovery rate is 85.5%.
Embodiment 2
[0016] Example 2: Rhodochrosite is taken from a mine in Yiyang, Hunan, and its composition characteristics are shown in Table 2.
[0017] Table 1 Chemical composition of rhodochrosite (%)
[0018] Element
[0019] Take 10Kg of rhodochrosite raw ore, after crushing and screening to obtain ore powder with a particle size of less than 25mm, carry out microwave roasting, the roasting temperature is 800°C, and the roasting time is 30 minutes; after the roasting is completed, add water to the ore powder, and wet grind until the particle size is less than 1mm , the solid mass concentration in the grinding process is 65%. The spiral chute is used to sort the grinding pulp to obtain manganese concentrate. The added water and the pulp are fed into the spiral chute at the same time during the sorting process. The solid mass concentration in the sorting process is The manganese grade in manganese concentrate is 23.5%, and the manganese recovery rate is 88.0%.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com