Aqueous demolding agent and production method thereof
A production method and release agent technology, which is applied in the field of water-based release agents for metal templates such as aluminum alloys and steel templates, can solve problems such as polluting the environment, affecting concrete structures, and dirty operations by workers, and achieves simple preparation processes and enhanced self-efficacy. Good raising ability and demoulding effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A water-based release agent, based on 100% by weight, containing 1% to 5% of polyvinyl alcohol, 0.02% to 0.06% of formaldehyde, 0.02% to 0.07% of borax, and 0.25% to 0.4% of sodium ethoxylated alkyl sulfate , 18 natural fatty alcohols 0%~0.5%, cetyltrimethylammonium chloride 0%~0.45%, the rest is made of water after batching and mixing, it is a milky white paste liquid, non-toxic and tasteless, Non-flammable.
[0014] In this embodiment, 3% of polyvinyl alcohol, 0.04% of formaldehyde, 0.05% of borax, 0.3% of sodium ethoxylated alkyl sulfate, 0% of octadecyl natural fatty alcohol, 0% of cetyltrimethylammonium chloride, The remainder is water 96.61%. The polyvinyl alcohol is PVA20-99(H).
[0015] A kind of production method of aqueous release agent is characterized in that it comprises the following steps:
[0016] ⑴Ingredients: By weight, take polyvinyl alcohol 1%~5%, formaldehyde 0.02%~0.06%, borax 0.02%~0.07%, ethoxylated sodium alkyl sulfate 0.25%~0.4%, eighteen na...
Embodiment 2
[0021] In order to increase the pasty effect of the product, the present embodiment takes 3% of polyvinyl alcohol, 0.04% of formaldehyde, 0.05% of borax, 0.3% of sodium ethoxylated alkyl sulfate, 0.3% of octadecyl natural fatty alcohol, cetyl tris Methyl ammonium chloride is 0.2% and the remainder is water 96.11%.
[0022] When preparing, first heat polyvinyl alcohol and water to 80°C to 95°C (90°C in this example) according to the proportioning ratio to dissolve, then add borax and stir to dissolve, after cooling to room temperature, add formaldehyde, sodium ethoxylated alkyl sulfate, Eighteen natural fatty alcohols and cetyltrimethylammonium chloride are stirred for 10 minutes to 15 minutes (15 minutes in this embodiment). The rest are the same as embodiment 1.
Embodiment 3
[0024] The present embodiment takes 1% of polyvinyl alcohol, 0.02% of formaldehyde, 0.02% of borax, 0.3% of ethoxylated alkyl sodium sulfate, 0.3% of octadecyl natural fatty alcohol, and 0.2% of cetyltrimethylammonium chloride. The rest is 98.16% of water. Remaining with embodiment 1, embodiment 2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com