Polymer, preparation method thereof and use method thereof
A polymer and sediment technology, applied in chemical instruments and methods, water/sludge/sewage treatment, flocculation/sedimentation water/sewage treatment, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0022] The preparation method of the polymer involved in the present invention may include: providing the inclusion formula A polymer of the IV structural unit, reacting the polymer comprising the structural unit of formula IV with ammonia, primary amine, secondary amine or tertiary amine to obtain a reactive polymer, and reacting the reactive polymer with carbon disulfide, hydrosulfide or sulfide to obtain form inclusive A polymer of I structural units, where R 1 selected from -SH, secondary, tertiary and quaternary amino groups, R 2 selected from hydrogen ion, NH 4 + , alkali metal ions and alkaline earth metal ions, R 3 Selected from Hydrogen and SSC-R 2 , X is a halogen.
[0023] In some embodiments, the hydrosulfide salt is sodium hydrosulfide. In some embodiments, X is chlorine. In some embodiments, the polymer comprising structural units of formula IV is obtained by polymerizing epichlorohydrin.
[0024] In another aspect, the present invention relates to a...
example 1
[0035]
[0036] Epichlorohydrin (50 grams) was slowly added to stirring 1 gram of concentrated phosphoric acid and 1 gram of deionized water between 90°C and 95°C. Then 1 gram of concentrated phosphoric acid and 50 grams of epichlorohydrin were added over a further 30 minutes. The product of this reaction is polyepichlorohydrin ( 1 H NMR (CDCl 3 ): 3.2~3.4(1H), 3.6~4.1(4H), 1.2(2H)), which were directly used in Example 2 without any purification or isolation.
example 2
[0038]
[0039] The polyepichlorohydrin (5 grams) that obtains in example 1 is slowly added the ammonia solution (concentration is 28%) of 10 grams, obtains-NH after this mixture is stirred gently 90 minutes 2 polymers as side groups, 1 H NMR (CDCl 3 ): 2.8~3.1(3H), 3.4~3.6(2H), 1.2(2H).
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com