A technology of negative ion fiber and production method, which is applied in the field of production of negative ion fiber air-conditioning grids, can solve the problems of unseen and inability to remove toxic gases, and achieve the functions of regulating central nervous system, strong sterilization and detoxification, and prevention of bacterial growth Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A method for making an anion fiber air-conditioning grid, comprising the following steps:
[0017] Step 1. Coating nano-slurry on the carbon fiber with a thickness of 0.6 mm, and evenly covering it with 3%-15% negative ion powder to obtain negative ion fibers;
[0018] Step 2, fully stir the bamboo charcoal powder and liquid titanium dioxide in the mixing tank, the stirring speed is 60 rpm, the stirring time is 20 minutes, and stir at normal temperature to generate agitated matter;
[0019] Step 3, evenly cover the mass of the agitated material on the prepared negative ion fiber in a proportion of 15%, to obtain mixed negative ion fiber;
[0020] Step 4, pave the mixed anion fibers, and then reinforce and bond the other side of the pavement to obtain viscose anion fibers;
[0021] Step 5. According to the size of the required air conditioner grid model, use machinery to judge the negative ion fiber of viscose, and carry out balanced concave and convex interfolding, glu...
Embodiment 2
[0026] The difference from Example 1 is: Step 1, coating nano-slurry on the carbon fiber with a thickness of 0.7mm, evenly covered with 8% negative ion powder; Step 2, the stirring speed is 65 rpm, and the stirring time is 25 minutes ; Step 3, evenly cover the mass of the agitated material on the negative ion fiber that has been produced in a proportion of 18%; Step 5, the width of the folded surface is 1.5cm.
[0027] The ratio specification of negative ion powder is: rare earth, 55%, tourmaline powder, 18%, lanthanide element, 25%.
[0028] The carbon fiber has a moisture content of 7% and a surface area of 450m 2 / g, dry carbon heat value is 3200kj / kg and pH value is 9
[0029] The rest are the same as in Embodiment 1, and will not be repeated here.
Embodiment 3
[0031] The difference from Example 2 is: Step 1, coating nano-slurry on the carbon fiber with a thickness of 0.8mm, evenly covered with 15% negative ion powder; Step 2, the stirring speed is 70 rpm, and the stirring time is 30 minutes ; Step 3, evenly cover the mass of the agitated material on the negative ion fibers that have been produced in a proportion of 20%; Step 5, the width of the folded surface is 2cm.
[0032] The ratio specification of negative ion powder is: rare earth, 60%, tourmaline powder, 20%, lanthanide element, 30%.
[0033] The carbon fiber has a moisture content of 8% and a surface area of 600m 2 / g and dry carbon heat value is 3300kj / kg
[0034] The rest are the same as in Embodiment 2, and will not be repeated here.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com