A manufacturing method and technology of tipping paper, applied in pulp beating method, special paper, paper, etc., can solve the problems of excessive absorption of glue, bursting of cigarettes, increased glue consumption, etc., to meet the requirements of high-speed work, fine texture, even paper effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Example 1: North American pine pulp and Indonesian acacia pulp were selected for beating respectively, the ratio of softwood pulp to hardwood pulp was 80:20; beating concentration control: 4.0%; blending degree of beating: 92 0 SR; Sizing amount: 3.5%, the main component of the sizing solution is acrylic compound. Finished transparent tipping paper physical index: Quantitative 50g / m 2 ; Tensile strength (longitudinal) 4.2kN / m; tearing degree (longitudinal and transverse average) 350mN; transparency 75%.
Embodiment 2
[0015] Example 2: North American pine pulp and Indonesian acacia pulp were selected for beating respectively, the pulp ratio of softwood pulp and hardwood pulp was 75:25; beating concentration control: 4.0%; beating degree of blended pulp: 90 0 SR; Sizing amount: 3.0%, the main component of the sizing solution is acrylic compound. Finished transparent tipping paper physical index: Quantitative 40g / m 2 ; Tensile strength (longitudinal) 3.5kN / m; tearing degree (longitudinal and transverse average) 280mN; transparency 80%.
Embodiment 3
[0016] Example 3: North American pine pulp and South American eucalyptus pulp were selected for beating respectively, the ratio of softwood pulp to hardwood pulp was 80:20; beating concentration control: 4.0%; blending degree of beating: 93 0 SR; Sizing amount: 4%, the main component of the sizing solution is acrylic compound. Finished transparent tipping paper physical index: Quantitative 50g / m 2 ; Tensile strength (longitudinal) 4.2kN / m; tearing degree (longitudinal and transverse average) 350mN; transparency 73%.
PUM
Property | Measurement | Unit |
---|---|---|
transparency | aaaaa | aaaaa |
transparency | aaaaa | aaaaa |
transparency | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com