[0018] A kind of preparation method of novel fuel, comprises the following steps:
[0019] (1) Mix 30% monoglyceride, 20-45% Span, 20% sodium dodecylbenzenesulfonate, 3% sodium carboxymethylcellulose (CMC), and 2% xanthan gum to obtain an emulsifier;
[0020] (2) Dissolve 5 kg of emulsifier in 175 kg of recovered oil, stir at 30°C and 4500 rpm, and emulsify for 30 minutes;
[0021] (3)然后在乳化液中加入煤粉含量占60%的水煤浆320公斤,搅拌转速为4500rpmrpm,搅拌时间为30min,混合均匀即得。
[0022] After testing, the finished product indicators are shown in the table below:
[0023] oily Moisture Ash Volatile matter Total sulfur low calorific value viscosity 35% 23.1 9.25 49.65 0.24 5605kcal / kg 1100
Embodiment 2
[0025] A kind of preparation method of novel fuel, comprises the following steps:
[0026] (1) Add 30% monoglyceride and 20-45% Span. Sodium lignosulfonate 20%, sodium carboxymethylcellulose (CMC) 3%, and xanthan gum 2% are mixed evenly to obtain an emulsifier;
[0027] (2) Dissolve 4 kg of emulsifier in 130 kg of recovered oil, stir at 45°C at a speed of 5500 rpm, and emulsify for 20 minutes;
[0028] (3) Then add 66 kg of coal-water slurry with a coal powder content of 60% to the emulsion, stir at a speed of 5500 rpm, and stir for 25 minutes, and mix evenly.
[0029] After testing, the finished product indicators are shown in the table below:
[0030] oily Moisture Ash Volatile matter Total sulfur low calorific value viscosity 65% 12.2 3.73 71.62 0.12 7482kcal / kg 500
Embodiment 3
[0032] A kind of preparation method of novel fuel, comprises the following steps:
[0033] (1) Mix 30% monoglyceride, 45% Span 20, 20% Tween 80, 3% sodium carboxymethylcellulose (CMC), and 2% xanthan gum to obtain an emulsifier;
[0034] (2) Dissolve 1.5kg of emulsifier in 50kg of recovered oil first, stir at 35°C and rotate at 5000rpm, and emulsify for 25min;
[0035] (3) Then add 48.5 kg of coal-water slurry with a coal powder content of 60% to the emulsion, the stirring speed is 4500rpmrpm, the stirring time is 20min, and the mixture is uniform.
[0036] After testing, the finished product indicators are shown in the table below:
[0037] oily Moisture Ash Volatile matter Total sulfur low calorific value viscosity 50% 16.0 11.35 60.85 0.20 5143kcal / kg 850
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com