Embodiment 1
[0022] How to prepare lavender natural incense:
[0023] In the first step, dehydrated lavender is pulverized to obtain lavender powder, and the pulverized particle size is 250 mesh;
[0024] In the second step, mix 40kg of lavender powder, 10kg of water hemp skin powder, 0.5kg of tea seed powder with an oil content of 10% and 30kg of lavender essence; among them, water hemp skin powder and tea seed powder are both 250 mesh in particle size .
[0025] In the third step, the above-mentioned mixed material is formed into a column shape with an incense forming machine;
[0026] The fourth step is drying and dehydration, so that the moisture content is 10%, and the finished product is obtained.
[0027] The dehydrated lavender and lavender essence in this example are prepared by the method disclosed in Example 1 of the Chinese invention patent CN 103045367 A applied by the applicant. Similarly, the dehydrated lavender and lavender essence prepared in other examples in Chinese i...
Embodiment 2
[0030] How to prepare lavender natural incense:
[0031] In the first step, dehydrated lavender is pulverized to obtain lavender powder, and the pulverized particle size is 300 mesh;
[0032] In the second step, mix 30kg of lavender powder, 8kg of water hemp skin powder, 0.3kg of tea seed powder with an oil content of 7% and 20kg of lavender essence; among them, water hemp skin powder and tea seed powder are both 300 mesh in particle size .
[0033] In the third step, use an incense molding machine to shape the above-mentioned mixed materials into sheets;
[0034] The fourth step is drying and dehydration, so that the moisture content is 8%, and the finished product is obtained.
[0035] The dehydrated lavender and lavender essence in this example are prepared by the method disclosed in Example 1 of the Chinese invention patent CN 103045367 A applied by the applicant. Similarly, the dehydrated lavender and lavender essence prepared in other examples in Chinese invention pat...
Embodiment 3
[0038] How to prepare lavender natural incense:
[0039] In the first step, dehydrated lavender is pulverized to obtain lavender powder, and the pulverized particle size is 200 mesh;
[0040] In the second step, mix 50kg of lavender powder, 12kg of water hemp skin powder, 0.6kg of tea seed powder with an oil content of 7% and 40kg of lavender essence; among them, water hemp skin powder and tea seed powder are both 200 mesh in particle size .
[0041] The third step is to use the incense molding machine to shape the above-mentioned mixed materials into a linear shape;
[0042] The fourth step is drying and dehydration, so that the moisture content is 12%, and the finished product is obtained.
[0043] The dehydrated lavender and lavender essence in this example are prepared by the method disclosed in Example 1 of the Chinese invention patent CN 103045367 A applied by the applicant. Similarly, the dehydrated lavender and lavender essence prepared in other examples in Chinese ...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com