[0028] Take 10% of graphene powder of 10 microns, 30% of loess, 20% of titanium dioxide powder of 10 microns, 20% of ferrite powder of 10 microns, 10% of ferrite permanent magnetic material powder of 10 microns, 100 Micron coconut shell activated carbon powder 10%.
[0029] The specific preparation method is to prepare the raw materials in the above weight percentage according to the following steps:
[0030] a) Put the loess in an oven for drying and sterilization, continue drying at 300°C for 6 hours, then grind it with a ball mill for 3 hours, pass through a 100 micron sieve, and prepare loess powder;
[0031] b) Pretreat the 10 micron ferrite powder with microwave heating for 1 hour, then pour it into the blender and stir while adding 10 micron titanium dioxide powder, stir evenly for 30 minutes, then add 10 micron ferrite permanent magnet material Powder, continue stirring for 30 minutes, then add 10 micron graphene powder, continue stirring for 30 minutes, finally add 1...
Embodiment 2
[0034] Take 5% of graphene powder of 5 microns, 20% of loess, 20% of tungsten trioxide powder of 5 microns, 20% of magnesium tourmaline powder of 5 microns, 20% of NdFeB material powder of 5 microns, 50 Micron bamboo activated carbon powder 15%.
[0035] The specific preparation method is to prepare the raw materials in the above weight percentage according to the following steps:
[0036] a) Put the loess in an oven for drying and sterilization, continue drying at 300°C for 6 hours, then grind it with a ball mill for 3 hours, pass through a 100 micron sieve, and prepare loess powder;
[0037] b) Pretreat 5-micron magnesium tourmaline powder with microwave heating for 1 hour, then pour it into a blender and stir while adding 5-micron tungsten trioxide powder, stir evenly for 30 minutes, then add 5-micron NdFeB Material powder, continue stirring for 30 minutes, then add 5 micron graphene powder, continue stirring for 30 minutes, finally add 50 micron bamboo activated carbon po...
Embodiment 3
[0040] Take 5 micron graphene powder 10%, 100 micron loess powder 20%, 10 micron tungsten trioxide powder 10%, 3 micron lithium tourmaline powder 30%, 10 micron samarium cobalt material powder 15%, 100 micron coal-based activated carbon powder 15%.
[0041] The specific preparation method is to prepare the raw materials in the above weight percentage according to the following steps:
[0042] a) Put the loess in an oven for drying and sterilization, continue drying at 300°C for 6 hours, then grind it with a ball mill for 3 hours, pass through a 100 micron sieve, and prepare loess powder;
[0043] b) Pretreat 3 micron lithium tourmaline powder with microwave heating for 1 hour, take the pretreated 3 micron lithium tourmaline powder and pour it into a blender, add 10 micron samarium cobalt material powder, and stir evenly for 30 Minutes later, add 10 microns of ferrite powder and continue stirring for 30 minutes, then add 5 microns of graphene powder, continue stirring for 30 m...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com