Method for processing high-iron low-tin ore
A technology for high iron and low tin ore and iron ore, which is applied in the field of processing high iron and low tin ores, can solve the problems that minerals cannot be effectively developed and utilized, cannot be separated, smelted and separated, and is difficult to develop and utilize, and achieves a simple and feasible method, scientific selection and high benefit. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A method for processing high-iron and low-tin ore, comprising: mixing high-iron and low-tin ore with reduced coal, pyrite, calcium chloride and carbon powder in a weight ratio of 1:0.8:0.6:0.055:0.5, using a disc ball making machine Make pellets, the diameter of the pellets is 14-24mm, put the pellets into a tunnel kiln, and bake the pellets at a temperature of 800°C for 8 hours. The volatilized tin is absorbed by the absorbent diatomaceous earth and converted into metallic tin , and finally get iron ore. The yields of iron and tin are both greater than 80%.
Embodiment 2
[0015] A method for processing high-iron and low-tin ore, comprising: mixing high-iron and low-tin ore with reduced coal, pyrite, calcium chloride and carbon powder in a weight ratio of 1:0.6:0.6:0.1:0.1, using a disc ball making machine Make pellets, the diameter of the pellets is 14-24mm, put the pellets into a tunnel kiln, and bake the pellets at a temperature of 1100°C for 5 hours. The volatilized tin is absorbed by the absorbent diatomaceous earth and converted into metallic tin , and finally get iron ore. The yields of iron and tin are both greater than 80%.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More