A technology of protective glue and peach glue, applied in the coating and other directions, can solve the problems of not extending the life of the printing plate, uneven protective film, reducing the protective effect, etc., and achieves easy washing, convenient printing, and good film formation. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0016] A special protective glue for PS / CTP plate, prepared from the following components by weight (kg): Gum Arabic 3, Peach Gum 3, Pineapple Pectin 1, Hydroxyethyl Fiber 4, Peppermint Essential Oil 0.15, Polyvinyl Alcohol 1.2, composite additive 2, deionized water 80,
[0017] Among them, the compound auxiliary agent is made of the following raw materials by weight (kg): sodium stearoyl lactylate 5, polyglycerol ester 4, coconut oil 3, fresh ginger juice 1, squalane 2, decyl glucoside 3.1, glycerin 5, Propylene glycol 7, lactic acid 1, polyvinyl ether 2, lavender essential oil 0.3, antioxidant 168 2, liquid paraffin 2, ethanol 9, ethyl acetate 9, propylene glycol alginate 5, water 14, the preparation method is: first ethanol and Mix ethyl acetate, then mix with squalane, decyl glucoside, glycerin, propylene glycol, lactic acid, antioxidant 168, heat to 60-70°C, stir for 30-40 minutes, then add other remaining ingredients, Raise the temperature to 75-80°C and stir at high sp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com