Preparation method for cadmium telluride

A technology of cadmium telluride and tellurium powder, which is applied in the direction of binary selenium/tellurium compounds, etc., can solve the problems of expensive quartz tubes, waste of materials, and increased costs, so as to improve the purity and utilization of raw materials, improve the purity and Productivity, the effect of saving production cost

Inactive Publication Date: 2014-05-28
张家港绿能新材料科技有限公司
View PDF3 Cites 9 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

This method adopts the method of heating with a hot rod, the temperature is not uniform enough, and the reaction is not sufficient
The Chinese invention patent with the publication number CN1380246A discloses a preparation method of pounded cadmium powder. The method uses cadmium powder and tellurium powder to synthesize in a crucible under vacuum conditions. The synthesis temperature is to react at the melting point of cadmium. After grinding and annealing, the disadvantage is that the synthesis rate is difficult to guarantee
The Chinese invention patent with the patent number of 200910312590.0 discloses a preparation method of high-purity cadmium telluride. This method is a synthesis reaction in a closed quartz tube coated with carbon, and the cadmium material and tellurium material are alternately put into the quartz tube according to the proportioning ratio. , deoxidize after charging, sinter and seal the tube with bubble sealing, and slowly carry out the synthesis reaction of high temperature and high pressure. Since the conditions of this method are high temperature and high pressure, there are certain risks in the synthesis process, and the industrialization cost is high.
The Chinese invention patent application with the publication number 103420346A discloses a preparation method of cadmium telluride. The method is to put tellurium powder and cadmium powder into the graphite boat in proportion, then place the graphite boat in the quartz tube, and then put the The graphite boat is placed in the synthesis furnace, and the multi-stage heating reaction is carried out first, and then the temperature is lowered in stages to complete the first synthesis, and then repeat the same steps for the second synthesis. This method requires cumbersome loading steps for each synthesis : Put graphite first, then quartz tube, and finally into the synthesis furnace
Moreover, it needs to use quartz tubes for feeding, deoxidation, sealing and breaking quartz tubes to take materials during the synthesis process. Quartz tubes are expensive and cannot be made into other shapes. Each charge is limited and cannot be mass-produced. All need a quartz tube, wasting materials and increasing costs

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0024] A preparation method of cadmium telluride, which sequentially comprises the following steps:

[0025] Take 10.638kg of qualified 5N tellurium powder and 9.376kg of 5N cadmium powder, pass the tellurium powder through a 100-mesh sieve, and pass the cadmium powder through a 200-mesh sieve, and check whether the tellurium powder and cadmium powder form agglomerates, and if there are agglomerates, crush them Sift again.

[0026] Put the above-prepared raw material tellurium powder and cadmium powder into a 20L polyurethane tank, cover the lid, and then load it into a homogenizer with a homogenization pressure of 9×101.325KPa.

[0027] Put the homogeneous mixed material into the graphite boat, then slowly put the loaded graphite boat into the synthesis, and place it in the middle of the synthesis furnace.

[0028] Cover the cap of the synthesis furnace, seal and fix it, then feed nitrogen gas, set the flow rate to 2 L / min, and the time to be 60 min.

[0029] The synthesis ...

Embodiment 2

[0043] A preparation method of cadmium telluride, which sequentially comprises the following steps:

[0044] Take 10.638kg of qualified 5N tellurium powder and 9.376kg of 5N cadmium powder, pass the tellurium powder through a 100-mesh sieve, and pass the cadmium powder through a 200-mesh sieve, and check whether the tellurium powder and cadmium powder form agglomerates, and if there are agglomerates, crush them Sift again.

[0045] Put the above-prepared raw material tellurium powder and cadmium powder into a 20L polyurethane tank, cover the lid, and then load it into a homogenizer with a homogenization pressure of 10×101.325KPa.

[0046] Put the homogeneous mixed material into the graphite boat, then slowly put the loaded graphite boat into the synthesis, and place it in the middle of the synthesis furnace.

[0047] Cover the cap of the synthesis furnace, seal and fix it, then feed nitrogen, set the flow rate to 5 L / min, and the time to be 40 min.

[0048] The synthesis fur...

Embodiment 3

[0062] A preparation method of cadmium telluride, which sequentially comprises the following steps:

[0063] Take 10.638kg of qualified 5N tellurium powder and 9.376kg of 5N cadmium powder, pass the tellurium powder through a 100-mesh sieve, and pass the cadmium powder through a 200-mesh sieve, and check whether the tellurium powder and cadmium powder form agglomerates, and if there are agglomerates, crush them Sift again.

[0064] Put the above-prepared raw material tellurium powder and cadmium powder into a 20L polyurethane tank, cover the lid, and then load it into a homogenizer with a homogenization pressure of 11×101.325KPa.

[0065] Put the homogeneous mixed material into the graphite boat, then slowly put the loaded graphite boat into the synthesis, and place it in the middle of the synthesis furnace.

[0066] Cover the cap of the synthesis furnace, seal and fix it, then feed nitrogen gas, set the flow rate to 2 L / min, and the time to be 60 min.

[0067] The synthesis...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
melting pointaaaaaaaaaa
Login to view more

Abstract

The invention discloses a preparation method for cadmium telluride. The preparation method sequentially comprises the following steps: qualified tellurium powder and cadmium powder are taken according to the molar ratio of 1:1 and then subjected to homogeneous mixing, the mixed raw materials subjected to homogenizing are loaded into a graphite boat, and the graphite boat is placed into a synthesis furnace for first synthesis; the material obtained after first synthesis is taken out of the graphite boat and crushed; the crushed material is loaded into the graphite boat, and the graphite boat is placed into the synthesis furnace for second synthesis; screening and ball milling are performed, wherein in the processes of the first synthesis and the second synthesis, multistage temperature rising and temperature dropping are performed under the protection of nitrogen and hydrogen. According to the invention, homogeneous treatment is performed on the tellurium powder and cadmium powder firstly so as to enable the two raw materials to be mixed fully and uniformly, meanwhile, the defect that the cadmium powder is easy to oxidize is overcome, the two raw materials can be synthesized preliminarily under relatively low temperature, purity of a synthesized product is improved, and the utilization ratios of raw materials are increased; synthesis is performed for two times, so that the raw materials react fully, thereby improving the purity and yield of the product finally.

Description

technical field [0001] The invention relates to the technical field of semiconductor materials, in particular to a preparation method of cadmium telluride. Background technique [0002] Cadmium telluride is a semiconductor compound synthesized by cadmium and tellurium. It is brown-black crystal powder, insoluble in water and acid, and can be decomposed by nitric acid. ideal photoelectric conversion material. [0003] At present, there are many ways to synthesize cadmium telluride. The earlier synthesis method of cadmium telluride is to insert a hot rod into the mixed powder of cadmium and cadmium, and heat it to 500°C to form it. This method adopts the mode of hot rod heating, and the temperature is not uniform enough, and the reaction is not sufficient enough. The Chinese invention patent with the publication number CN1380246A discloses a preparation method of pounded cadmium powder. The method uses cadmium powder and tellurium powder to synthesize in a crucible under vac...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C01B19/04
Inventor 梁文正
Owner 张家港绿能新材料科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products