Matte-underglazed glazed brick and fabrication process thereof
A production process and technology for polishing glazed tiles, applied in the field of ceramic tile production, can solve the problems of insufficient glaze, insufficient delicacy, poor matte effect, etc., and achieve the effect of smooth and delicate surface
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] The manufacturing process of the matt underglaze color-polished glazed brick in the present embodiment comprises the following steps:
[0036] 1. Choose white low water absorption finished adobe as the bottom brick;
[0037] 2. Design various patterns according to the needs, and make them into screens for printing;
[0038] 3. Clean the surface of the bottom brick, and use an automatic printing machine to print patterns of different colors and effects on the bottom brick;
[0039] 4. Cover the bricks with different patterns on the printed bricks;
[0040] The composition of the frit meets the following requirements:
[0041] AL 2 o 3 : 6%, SiO 2 : 64%, Fe 2 o 3 : 2 O: 2%, Na 2 O: 4%, TiO 2 : 2 o 3 : 12%, PbO: 2 : 2O: <0.05%, loss on ignition: <0.05%.
[0042] 5. Bricks printed with patterns and covered with frit layer are fired in a kiln at a temperature of 970°C. After about one and a half hours of firing, the frit on the surface is fused into a transparent ...
Embodiment 2
[0048] The manufacturing process of the matt underglaze color-polished glazed brick in the present embodiment comprises the following steps:
[0049] 1. Choose white low water absorption finished adobe as the bottom brick;
[0050] 2. Design various patterns according to the needs, and make them into screens for printing;
[0051] 3. Clean the surface of the bottom brick, and use an automatic printing machine to print patterns of different colors and effects on the bottom brick;
[0052] 4. Cover the bricks with different patterns on the printed bricks;
[0053] The composition of the frit meets the following requirements:
[0054] AL 2 o 3 : 7%, SiO 2 : 63%, Fe 2 o 3 : 2 O: 2%, Na 2 O: 3%, TiO 2 : 2 o 3 : 13%, PbO: 2 : 2 O: <0.05%, loss on ignition: <0.05%.
[0055] 5. Bricks printed with patterns and covered with frit layer are fired in a kiln at a temperature of 975°C. After about one and a half hours of firing, the frit on the surface is fused into a transparent...
Embodiment 3
[0061] The manufacturing process of the matt underglaze color-polished glazed brick in the present embodiment comprises the following steps:
[0062] 1. Choose white low water absorption finished adobe as the bottom brick;
[0063] 2. Design various patterns according to the needs, and make them into screens for printing;
[0064] 3. Clean the surface of the bottom brick, and use an automatic printing machine to print patterns of different colors and effects on the bottom brick;
[0065] 4. Cover the bricks with different patterns on the printed bricks;
[0066] The composition of the frit meets the following requirements:
[0067] AL 2 o 3 : 9%, SiO 2 : 66%, Fe 2 o 3 : 2 O: 2%, Na 2 O: 3%, TiO 2 : 2 o 3 : 13%, PbO: 2 : 2 O: <0.05%, loss on ignition: <0.05%.
[0068] 5. Bricks printed with flowers and covered with frit layer are fired in a kiln at a temperature of 980°C. After about one and a half hours of firing, the frit on the surface is fused into a transparent ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com