Embodiment 1
[0051] The isopropanol of 40g, the n-butyl acetate of 5g are mixed, the BT-828 type organic bentonite of 4.5g is added in the obtained mixture and carry out the first mixing, obtain the first mixture of fineness≤45 microns; Add 50 g of BT-1826 zinc stearate and 0.5 g of HX-2500 type defoamer to the mixture and carry out the second mixing for 10 minutes to obtain the colored base.
[0052] The colored base material obtained in Example 1 of the present invention and the colored paint of forest green color are mixed according to the ratio of 7:3 in mass ratio to obtain colored pigment, and the colored paint of described forest green color is made of NC green primer and Shiming brand The color paste of SUP-8004 is formulated according to the mass ratio of 88:12;
[0053] Spraying the above-mentioned coloring pigment on the surface of the wood material after polishing the wood material;
[0054] After the coloring pigment on the surface of the wood material is dried, the surface o...
Embodiment 2
[0057] Mix 30g of isopropanol and 3g of methyl isobutyl ketone, add 2g of BT-828 type organobentonite to the resulting mixture for the first mixing to obtain a first mixture with a fineness≤45 microns; Add 30 g of BT-1826 zinc stearate and 0.2 g of HX-2500 type defoamer to the first mixture for 10 minutes of second mixing to obtain a colored base.
[0058] According to the method described in Example 1, the colored base material prepared in Example 2 of the present invention was used to prepare a forest green woody material.
[0059] According to the method described in Example 1, the forest green woody material prepared in Example 2 of the present invention is detected, and the detection result is that the color degree of the forest green woody material obtained in Example 2 of the present invention is 33, and the color is old, which is the same as that in Example 1. The chromaticity 35 of described forest green wooden sample is close; The channel clarity and color layering o...
Embodiment 3
[0061] Mix 60g of isopropanol and 20g of n-butyl acetate, add 10g of BT-828 type organobentonite to the resulting mixture and carry out the first mixing to obtain the first mixture with a fineness≤45 microns; to the first Add 60 g of BT-1826 zinc stearate and 0.8 g of HX-2500 type defoamer to the mixture and carry out the second mixing for 10 minutes to obtain the colored base.
[0062] According to the method described in Example 1, the colored base material prepared in Example 3 of the present invention was used to prepare a forest green woody material.
[0063] According to the method described in Example 1, the forest green woody material prepared in Example 3 of the present invention is detected, and the detection result is that the color degree of the forest green woody material obtained in Example 3 of the present invention is 34, and the color is old, which is the same as that in Example 1. The chromaticity 35 of described forest green wood sample is close; the channel...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com