High-adhesion ink for external package and preparation method thereof

A high-adhesion and outer-packaging technology, applied in the field of ink, can solve the problems of easy fading, poor adhesion, and affect the appearance, and achieves the effect of superior performance, ingenious ratio, and not easy to fade.

Inactive Publication Date: 2014-12-17
JURONG GEILI PACKAGING PROD FACTORY
View PDF2 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Many existing inks have poor adhesion and are prone to water loss, especially the inks used for outer packaging products, which are easy to fall off and fade over time, affecting the appearance

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0013] A kind of high-adhesion ink for outer packaging of the present invention is characterized in that: it comprises the following components in parts by weight: 6 parts of carbon black, 110 parts of deionized water, 1 part of gum arabic, 1 part of glycerin, 1 part of ethylene glycol 1 part, 3 parts of acrylic resin, 0.1 part of phenol, 9 parts of glucose, and 1 part of acetic acid.

[0014] The preparation method of the high-adhesion ink for outer packaging in the present embodiment may further comprise the steps:

[0015] (1) Put carbon black and gum arabic into ~8 parts by weight of deionized water, stir and grind for 1 hour;

[0016] (2) Stir and mix glycerin, ethylene glycol acrylic resin, phenol, glucose and acetic acid for 10 minutes;

[0017] (3) Pour the two solutions obtained in step (1) and step (2) into the remaining deionized water, then fully stir and grind for 30 minutes, and finally let the solution stand for 1 day, and the obtained clear liquid is high adhe...

Embodiment 2

[0019] A high-adhesion ink for outer packaging of the present invention comprises the following components in parts by weight: 9 parts of carbon black, 125 parts of deionized water, 3 parts of gum arabic, 3 parts of glycerin, 5 parts of ethylene glycol, acrylic resin 7 parts, 0.3 parts of phenol, 10 parts of glucose, 9 parts of acetic acid.

[0020] The preparation method of the high-adhesion ink for outer packaging of this embodiment is the same as that of Embodiment 1.

Embodiment 3

[0022] A high-adhesion ink for outer packaging of the present invention comprises the following components in parts by weight: 8.8 parts of carbon black, 123 parts of deionized water, 2.7 parts of gum arabic, 2.4 parts of glycerin, 4.5 parts of ethylene glycol, acrylic resin 6.5 parts, 0.26 parts of phenol, 9.9 parts of glucose, and 8 parts of B.

[0023] The preparation method of the high-adhesion ink for outer packaging of this embodiment is the same as that of Embodiment 1.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses high-adhesion ink for external package. The high-adhesion ink comprises the following components: carbon black, deionized water, Arabic gum, glycerinum, ethylene glycol, acrylic resin, phenol, glucose and acetic acid. The high-adhesion ink disclosed by the invention is excellent in property and high in adhesion, is not easily faded after being used for external package, and ingenious in matching ratio; and a preparation method of the high-adhesion ink is simple and easy to operate.

Description

technical field [0001] The invention relates to an ink, in particular to a high-adhesion ink for outer packaging and a preparation method thereof. Background technique [0002] Many existing inks have poor adhesion and are prone to water loss, especially the inks used for outer packaging products, which are very easy to fall off and fade over time, affecting the appearance. Contents of the invention [0003] Purpose of the invention: the purpose of the present invention is to solve the deficiencies in the prior art, to provide a kind of high adhesion ink for outer packaging and its preparation method. [0004] Technical solution: A high-adhesion ink for outer packaging of the present invention comprises the following components in parts by weight: 6-9 parts of carbon black, 110-125 parts of deionized water, 1-3 parts of gum arabic, 1-3 parts of glycerin 3 parts, ethylene glycol 1~5 parts, acrylic resin 3~7 parts, phenol 0.1~0.3 parts, glucose 9~10 parts, acetic acid 1~9 ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D11/00
Inventor 潘冬生
Owner JURONG GEILI PACKAGING PROD FACTORY
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products