Eureka AIR delivers breakthrough ideas for toughest innovation challenges, trusted by R&D personnel around the world.

Method for imitating white fox skin with blue fox skin

A technology of blue fox fur and white fox fur, which is applied in the field of animal fur treatment, can solve the problems of white fox fur not pure enough, low quality of white fox fur, and large amount of hydrogen peroxide, and achieve the effect of pure white, high quality, and small amount of hydrogen peroxide

Active Publication Date: 2016-06-29
BEIJING FANBO CHEM
View PDF3 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] The current method of imitating white fox fur for blue fox fur uses a large amount of hydrogen peroxide for processing, and the white color of the obtained white fox fur is not pure enough, the hair quality is greatly damaged, and the quality of the obtained white fox fur is low.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0039] The method for blue fox skin imitation white fox skin comprises the following steps:

[0040] (1) Select the raw skin, the selected blue fox skin has not been dyed, and remove the defects such as depilation, messy guard hair, knot hair, dead hair, tortoise hair, broken board, rotten board and so on. the fur;

[0041] (2) Treatment of guard hair: Brush Weijia Iced Tea Agent B on the tip of the blue fox fur, and let it stand for 6 hours;

[0042] (3), medium: the blue fox fur after the guard hair is soaked in the first mixed aqueous solution; wherein, in terms of water volume, the first mixed aqueous solution contains salt 35g / L, Eliite wetting agent HAC0. 4ml / L and ferrous sulfate 12g / L, and adjust the pH value to 3.9 with acetic acid;

[0043] The temperature of soaking is 30°C, and the time is 20 hours; after soaking, peel off the skin, shake off the water, and proceed to the next step of bleaching;

[0044] (4), bleaching: adopt the second mixed aqueous solution to c...

Embodiment 2

[0054] The method for blue fox skin imitation white fox skin comprises the following steps:

[0055] (1) Select the raw skin, the selected blue fox skin has not been dyed, and remove the defects such as depilation, messy guard hair, knot hair, dead hair, tortoise hair, broken board, rotten board and so on. the fur;

[0056] (2) Treatment of guard hair: Mix Weijia Iced Tea Agent B and water at a volume ratio of 0.5, then brush it on the tip of the blue fox fur, and let the hair stand for 15 hours;

[0057] (3), medium: the blue fox fur after the guard hair is soaked in the first mixed aqueous solution; wherein, in terms of water volume, the first mixed aqueous solution contains salt 40g / L, Eliite wetting agent HAC0. 5ml / L and ferrous sulfate 15g / L, and adjust the pH value to 4.0 with acetic acid;

[0058] The temperature of soaking is 32°C, and the time is 15 hours; after soaking, peel off the skin, shake off the water, and proceed to the next step of bleaching;

[0059] (4)...

Embodiment 3

[0069] The method for blue fox skin imitation white fox skin comprises the following steps:

[0070] (1) Select the raw skin, the selected blue fox skin has not been dyed, and remove the defects such as depilation, messy guard hair, knot hair, dead hair, tortoise hair, broken board, rotten board and so on. the fur;

[0071] (2) Treatment of guard hair: Mix Weijia Iced Tea Agent B and water at a volume ratio of 1, then brush it on the tip of the blue fox fur, and let the hair stand for 20 hours;

[0072] (3), medium: the blue fox fur after the guard hair is soaked in the first mixed aqueous solution; wherein, in terms of water volume, the first mixed aqueous solution contains salt 45g / L, Eliite wetting agent HAC0. 6ml / L and ferrous sulfate 17g / L, and adjust the pH value to 4.1 with acetic acid;

[0073] The temperature of soaking is 35°C, and the time is 12 hours; after soaking, peel off the skin, shake off the water, and proceed to the next step of bleaching;

[0074] (4), ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to the field of animal fur treatment, in particular to a method for imitating white fox fur from blue fox fur. , wetting agent and ferrous sulfate mixed solution soaking; hydrogen peroxide and other substances mixed solution for bleaching; and then after deferrification, reduction whitening, retanning and fatliquoring, drying. The method for imitating white fox fur of blue fox fur provided by the present invention first treats the tip of the guard hair of blue fox fur with Weijia iced tea agent B, so that the scale layer of the guard hair of blue fox fur is more thoroughly opened, and then undergoes specific Medium treatment, and then use hydrogen peroxide to bleach with other substances. The amount of hydrogen peroxide used is small. Through gradual bleaching, the purpose of hair protection is achieved, and the best bleaching effect of bleaching without harming the hair is achieved. The final white fox fur obtained is pure white, with less damage to the quilt, and the white fox fur imitated by the blue fox fur is more realistic, the quilt has a more three-dimensional effect, and is of high quality.

Description

technical field [0001] The invention relates to the field of animal fur treatment, in particular to a method for imitating white fox fur from blue fox fur. Background technique [0002] At present, the fashion of fur products is getting stronger and stronger, and there are more and more popular designs and colors. With the gradual expansion of the fur market, the continuous development and improvement of fur chemical industry, the product grades are rising step by step, and the varieties of designs and colors are emerging in an endless stream. The increasingly mature and developing clothing industry leads the trend of fashion life, providing unlimited business opportunities for the fur processing industry. Higher requirements are also put forward for fur dyeing and finishing. The fur processing industry relies on the technological progress of the fur chemical industry to occupy an increasingly important position in the colorful clothing industry. The characteristics of fur ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): D06L3/02D06L3/10D06M11/13D06M11/55C14C3/02C14C3/16C14C3/06C14C9/02D06M101/10D06L4/12D06L4/13
Inventor 吴涛郑超斌郑红超郝安生
Owner BEIJING FANBO CHEM
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Eureka Blog
Learn More
PatSnap group products