[0075] A super-flexible and super-tough household paper, including the following raw materials by weight:
[0076] 80 parts of slurry
[0077] Oil 5 parts
[0078] Polyol 4 parts
[0079] 3 parts of non-ionic surfactant
[0080] Softener 3 parts
[0081] Toughened fiber 3 parts
[0082] Dry strength agent 1 part
[0083] 1 part of wet strength agent;
[0084] Wherein, the softening agent is a mixture composed of glyceryl stearate, diethylene triamine and dimethyl sulfate in a weight ratio of 1.2:1:1.6;
[0085] The toughened fiber is a mixture composed of glass fiber, carbon fiber and ceramic fiber in a weight ratio of 1:0.8:1.5.
[0086] The slurry is a mixture composed of long fibers and short fibers in a weight ratio of 1.5:1.
[0087] The oil agent includes the following raw materials in weight percentages: (Z)-9-octadecenoic acid-dodecyl ester 40%, disodium laureth sulfosuccinate 20%, and coconut fatty acid, The reaction product of diethylenediamine, soybean fatty acid ethoxylate and qua...
Embodiment 2
[0102] A super-flexible and super-tough household paper, including the following raw materials by weight:
[0103] 90 parts of slurry
[0104] 6 parts oil
[0105] Polyol 5 parts
[0106] Non-ionic surface active agent 4 parts
[0107] Softener 4 parts
[0108] Toughened fiber 4 parts
[0109] Dry strength agent 4 parts
[0110] 4 parts of wet strength agent;
[0111] Wherein, the softening agent is a mixture composed of glyceryl stearate, diethylene triamine and dimethyl sulfate in a weight ratio of 1.3:1:1.8;
[0112] The toughened fiber is a mixture composed of glass fiber, carbon fiber and ceramic fiber in a weight ratio of 1:0.9:1.7.
[0113] The slurry is a mixture composed of long fibers and short fibers in a weight ratio of 1.7:1.
[0114] The oil agent includes the following raw materials in weight percentage: (Z)-9-octadecenoic acid-lauryl ester 45%, disodium laureth sulfosuccinate 22%, and coconut fatty acid, 22% of the reaction product of diethylenediamine, soybean fatty acid etho...
Embodiment 3
[0129] A super-flexible and super-tough household paper, including the following raw materials by weight:
[0130] 100 parts of slurry
[0131] 7 parts oil
[0132] Polyol 6 parts
[0133] Non-ionic surfactant 5 parts
[0134] Softener 5 parts
[0135] Toughened fiber 5 parts
[0136] Dry strength agent 3 parts
[0137] 3 parts of wet strength agent;
[0138] Wherein, the softening agent is a mixture composed of glyceryl stearate, diethylene triamine and dimethyl sulfate in a weight ratio of 1.5:1:2;
[0139] The toughened fiber is a mixture composed of glass fiber, carbon fiber and ceramic fiber in a weight ratio of 1:1:2.
[0140] The slurry is a mixture composed of long fibers and short fibers in a weight ratio of 2:1.
[0141] The oil agent includes the following raw materials in weight percentage: (Z)-9-octadecenoic acid-dodecyl ester 50%, disodium laureth sulfosuccinate 25%, and coconut fatty acid, 25% of the reaction product of diethylenediamine, soybean fatty acid ethoxylate and quate...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com