Preparation method of garbage incineration power generation furnace slag concrete
A waste incineration and concrete technology, which is applied in sustainable waste treatment, solid waste management, climate sustainability, etc., can solve the problem of insufficient mixing of waste slag concrete, gaps in concrete water resistance and compressive strength, stability and stability. Overall performance is not high
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 7
[0087] Example 7 The dosage ratio of each material in the concrete is based on the mass of the material required to prepare each cubic concrete, and is: 400kg of incineration power plant slag, 300kg of cement, 150kg of magnetized water, 260kg of sand, 1300kg of graded gravel with a particle size of 10-20mm, 3.3kg of water reducing agent, 20kg of GCY activator and 4kg of acrylic resin; the preparation method is as follows:
[0088] (1) Slag pretreatment: The slag discharged from the waste incineration boiler of the waste incineration power plant is washed by a hydrolysis tank to remove soluble salts, and then crushed and screened, magnetically separated, buoyantly sorted, and sieved to obtain a particle size of 3~ 5mm, the apparent density is 1996kg / m 3 waste slag coarse aggregate;
[0089] (2) Preparation of magnetized water: Use a magnetizer to magnetize tap water in advance to obtain magnetized water for use as a spare;
[0090] (3) Concrete preparation: first add 25% mag...
Embodiment 8
[0091] Example 8 The dosage ratio of each material in concrete is based on the mass of the material required to prepare each cubic concrete, which is: the dosage ratio of each material in the concrete, and is calculated as: garbage 250kg of incineration power plant slag, 550kg of cement, 200kg of magnetized water, 220kg of sand, 1100kg of graded gravel with a particle size of 10-20mm, 4kg of water reducing agent, 15kg of GCY activator and 4kg of acrylic resin; the preparation method is as follows:
[0092] (1) Slag pretreatment: The slag discharged from the waste incineration boiler of the waste incineration power plant is washed by a hydrolysis tank to remove soluble salts, and then crushed and screened, magnetically separated, buoyantly sorted, and sieved to obtain a particle size of 3~ 5mm, the apparent density is 1996kg / m 3 waste slag coarse aggregate;
[0093] (2) Preparation of magnetized water: Use a magnetizer to magnetize tap water in advance to obtain magnetized wa...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Apparent density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com