Nano-modified polymer material for table tennis and manufacturing method thereof

A polymer material and nano-modification technology, applied in the field of nano-modified polymer materials for table tennis and its manufacturing, can solve problems such as transportation and production difficulties, environmental hazards, and environmental hazards, and achieve various performance indicators Excellent, safe production, and less environmental pollution

Inactive Publication Date: 2015-11-04
浙江曙光体育用品有限公司
View PDF3 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Most table tennis balls in the prior art are manufactured using celluloid as a raw material. Although the table tennis balls made of celluloid have excellent performance, celluloid is flammable and explosive, difficult to transport and produce, and has a low safety factor. At the same time, its manufacturing cost is relatively high. , the process is more complicated, and the harm to the environment is greater
There are also a number of new materials that replace celluloid in the market, but these new materials generally do not meet the performance level of celluloid, and the manufacturing cost remains high. Materials with low environmental hazards and performance comparable to or exceeding that of celluloid are the difficulties that all personnel in the field of table tennis manufacturing need to overcome.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0018] A kind of nano-modified macromolecule material for table tennis, the main component of said material comprises by mass fraction ratio:

[0019] 50-75% polybutylene succinate or polylactic acid; 3%-7% lignin fiber; 1%-2% plant fiber; 15-18% plasticizer; 0.5-3% Titanium dioxide and silica nanomaterials. The material also includes polyvinyl chloride and polypropylene nano micropowder, and the total mass fraction thereof is 0.5-8%. The ingredients of the plasticizer include: butylene benzoate. Other common plasticizers can also be used.

Embodiment 2

[0021] The material components include by mass percentage: polyvinyl chloride: 2%; polypropylene nano-powder: 6%;

[0022] Polybutylene succinate or polylactic acid: 65%; lignin fibers: 5%; plant fibers: 2%; plasticizers: 17%; titanium dioxide nanomaterials: 1% silica nanomaterials: 2%.

Embodiment 3

[0024] Above-mentioned a kind of manufacture method of nano-modified polymer material for table tennis, the steps are as follows:

[0025] In the first step, the raw materials are mixed, according to the proportion of the main components in claim 1, mixed according to the mass fraction, and at the same time, 0.5% of the polyvinyl chloride and polypropylene nano-powder mixture is added, and stirred for 1-1.5h.

[0026] In the second step, the extruder is extruded into a sheet; the temperature range of the barrel of the extruder is 100-120 degrees, and the temperature of the plasticizing zone is 180-190 degrees.

[0027] In the third step, the cutting machine cuts the sheet into small pieces for table tennis manufacturing.

[0028] The nano-modified polymer material for table tennis provided by the invention has the advantages of safe production, biodegradability and less environmental pollution compared with celluloid materials. More than celluloid.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a nano-modified polymer material for table tennis. The nano-modified polymer material comprises, by weight, 50-75% of poly(butylene succinate) or polylactic acid; 3-7% of lignocelluloses, 1-2% of plant fibre, 15-18% of a plasticizer and 0.5-3% of titanium dioxide and nano-silica dioxide material. A manufacturing method of the nano-modified polymer material comprises the following steps: Step 1, mixing raw materials while adding 0.5% of a mixture of polyvinyl chloride and polypropylene nano-powders, and stirring for 1-1.5 h; Step 2, extruding by an extruder to obtain a sheet material; and Step 3, cutting the sheet material by a cutting machine into small pieces for manufacturing of table tennis. In comparison with a celluloid material, the nano-modified polymer material for table tennis is safe in production, is biodegradable and causes little environmental pollution. Meanwhile, table tennis prepared from the nano-modified polymer material has excellent performance indexes, and part of the performance exceeds performance of table tennis prepared from celluloid.

Description

technical field [0001] The invention specifically relates to the technical field of sporting goods, in particular to a nano-modified polymer material for table tennis and a manufacturing method thereof. Background technique [0002] Most table tennis balls in the prior art are manufactured using celluloid as a raw material. Although the table tennis balls made of celluloid have excellent performance, celluloid is flammable and explosive, difficult to transport and produce, and has a low safety factor. At the same time, its manufacturing cost is relatively high. , the process is more complicated, and the harm to the environment is greater. There are also a number of new materials that replace celluloid in the market, but these new materials generally do not meet the performance level of celluloid, and the manufacturing cost remains high. Materials with low environmental hazards and performance comparable to or exceeding that of celluloid are the difficulties that all personn...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C08L67/02C08L67/04C08L97/00C08L97/02C08L27/06C08L23/12C08K3/22C08K3/36C08K5/12
Inventor 陈伟立胡永汉包爱军
Owner 浙江曙光体育用品有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products