Manufacturing method for dyeing and printing sheep wool comforter
A production method and technology of sheep wool, applied in dyeing, textiles and papermaking, etc., can solve the problems of durability, practicability, and warmth retention, and achieve the effect of brilliant colors and extended application space
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] Example 1, In this embodiment, the background color of the fur quilt is black, and then the black line leopard pattern is printed.
[0047] 1. Preparation of blank leather before discharging
[0048] Select the white shearing blank leather with moderate hair density and proceed according to the existing conventional process steps: blank leather shearing, brushing, scalding, shearing, brushing formic acid solution, scalding, shearing, weighing, chrome retanning, standing, Degreasing, dyeing, washing, drying, regaining moisture, stretching, tensioning, placing, brushing with formic acid solution, scalding, shearing, shearing length is 1.0cm; 30 skins weighing 18kg, as the basis for the subsequent process materials.
[0049] 2. Spray color liquid
[0050] Equipment: wooden case, palm brush; material: color drawing liquid;
[0051] Dispensing liquid: Weigh thickener AA67.5g, pour it into 2183g water and stir evenly, then weigh discharge agent B-ST2250g into the thickening liquid and...
Embodiment 2
[0086] Example 2 In this embodiment, the background color is silver gray fur quilt, and the black line checkers pattern is directly printed.
[0087] 1. Preparation of blank leather before printing; proceed according to the existing conventional process steps: blank leather shearing, brushing, scalding, shearing, brushing formic acid solution, scalding, shearing, weighing, chrome retanning, standing, degreasing, dyeing , Washing, drying, re-moisture, stretching, stretching, placing, brushing with formic acid solution, scalding, shearing; shearing length is 0.8cm; 30 skins weighing 18kg, as the basis for subsequent processes.
[0088] 2. Printing; equipment: printing plate, scraper; material: thickener C-404%, dye 3%, fixing agent SLO3%, formic acid 10% and water 80%;
[0089] Dye paste: the same as in Example 1;
[0090] Printing operation method: the average material used for each piece of leather is 175g; the rest are the same as in Example 1.
[0091] 3. Steaming; equipment: steam...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com