A communication machine room, antirust paint technology, applied in the field of paint preparation, can solve the problems of large amount of addition, antistatic agent temperature resistance, water resistance, oil resistance, corrosion resistance and durability, high density of metal powder, etc., to achieve sustainable Long time, meet the effect of antistatic, good compatibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A kind of antistatic paint, it is made up of the material of following parts by weight:
[0020] 2 parts of sodium borate, 10 parts of phthalate, 5 parts of modified poly(3,4-ethylenedioxythiophene)-polystyrenesulfonic acid, 15 parts of aromatic polyurethane acrylate, 10 parts of silicone resin, 10 parts of dimethylaminoethyl acrylate, 45 parts of diluent, 0.5 part of leveling agent, 15 parts of graphene, 5 parts of magnesium chloride, 5 parts of nano-silver powder, 8 parts of polyvinylpyrrolidone, and 0.5 part of organic bentonite.
[0021] The preparation method of the modified poly(3,4-ethylenedioxythiophene)-polystyrenesulfonic acid is as follows:
[0022] At a temperature of 35°C, disperse sulfonated graphene, 3,4-ethylenedioxythiophene and polyethylene glycol in deionized water, so that the concentration of polyethylene glycol contained in the formed mixed system is 0.05 wt%, and sulfonated graphene, 3,4-ethylenedioxythiophene, the mass ratio of polyethylene glyc...
Embodiment 2
[0031] A kind of antistatic paint, it is made up of the material of following parts by weight:
[0032] 3 parts of sodium borate, 15 parts of phthalate, 8 parts of modified poly(3,4-ethylenedioxythiophene)-polystyrenesulfonic acid, 20 parts of aromatic polyurethane acrylate, 13 parts of silicone resin, 15 parts of dimethylaminoethyl acrylate, 50 parts of diluent, 0.8 part of leveling agent, 20 parts of graphene, 7 parts of magnesium chloride, 7 parts of nano-silver powder, 10 parts of polyvinylpyrrolidone, and 0.8 part of organic bentonite.
[0033] The preparation method of the modified poly(3,4-ethylenedioxythiophene)-polystyrenesulfonic acid is as follows:
[0034]At a temperature of 35°C, disperse sulfonated graphene, 3,4-ethylenedioxythiophene and polyethylene glycol in deionized water, so that the concentration of polyethylene glycol contained in the formed mixed system is 0.05 wt%, and sulfonated graphene, 3,4-ethylenedioxythiophene, the mass ratio of polyethylene glyc...
PUM
Property | Measurement | Unit |
---|---|---|
hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com