Unlock instant, AI-driven research and patent intelligence for your innovation.

Badminton seat outer layer reinforcement adhesive formula and production process thereof

A technology for reinforcing rubber and badminton, which is applied in the direction of adhesives, adhesive additives, natural rubber adhesives, etc., can solve the problems of badminton seat surface hardening, inability to play a protective role, racket damage, etc., to increase firmness and Compactness, reduce pollution and damage to human health, and prolong service life

Inactive Publication Date: 2016-08-31
安徽太阳体育用品有限公司
View PDF4 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] In the badminton production process, the seat part of the produced shuttlecock needs to be reinforced twice to ensure the firmness between the ball seat and the feather and the impact resistance of the ball seat. Generally, it is sprayed or soaked in reinforcement glue. When the technical reinforcement glue is used to reinforce the badminton seat, it often causes the surface of the badminton seat to harden and crack during the hitting process, which cannot provide the proper protection and also cause certain damage to the racket. , in the reinforcement of the outer layer of the badminton seat, a reinforcing glue that can not only increase the firmness between the seat and the feathers, but also increase the softness, compactness and durability of the seat

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] A kind of badminton seat outer reinforcing glue formula, the formula of described reinforcing glue comprises the following raw materials by weight: 10 parts of turpentine, 10 parts of rapeseed oil cake, 10 parts of animal fat, 6 parts of attapulgite powder, 6 parts of natural rubber, 8 parts cornstarch;

[0018] A production process of badminton seat outer layer reinforcing glue is prepared according to the following steps through the above-mentioned raw material formula in parts by weight:

[0019] 1) The rapeseed oil cake and natural rubber are stirred and pulverized by a stirring pulverizer to prepare a mixture for subsequent use;

[0020] 2) Pass pine resin and animal fat through a sealed container, heat and melt, and stir and mix. The heating temperature is 200-230° C., and the heating time is 90-120 minutes, and the mixed oil is prepared for use;

[0021] 3) Add the above-mentioned mixed oil into a sealed container, add the mixed material, and at the same time ad...

Embodiment 2

[0023] A kind of badminton seat outer layer reinforcement glue formula, the formula of described reinforcement glue comprises the following raw materials by weight: 12 parts of turpentine, 13 parts of rapeseed oil cake, 12 parts of animal fat, 8 parts of attapulgite powder, 7 parts of natural rubber, 10 parts cornstarch;

[0024] A production process of badminton seat outer layer reinforcing glue is prepared according to the following steps through the above-mentioned raw material formula in parts by weight:

[0025] 1) The rapeseed oil cake and natural rubber are stirred and pulverized by a stirring pulverizer to prepare a mixture for subsequent use;

[0026] 2) Pass pine resin and animal fat through a sealed container, heat and melt, and stir and mix. The heating temperature is 200-230° C., and the heating time is 90-120 minutes, and the mixed oil is prepared for use;

[0027] 3) Add the above-mentioned mixed oil into a sealed container, add the mixed material, and at the s...

Embodiment 3

[0029] A kind of badminton seat outer layer reinforcing glue formula, the formula of described reinforcing glue comprises the following raw materials by weight: 15 parts of turpentine, 15 parts of rapeseed oil cake, 15 parts of animal fat, 10 parts of attapulgite powder, 10 parts of natural rubber, 12 parts of cornstarch.

[0030] A production process of badminton seat outer layer reinforcing glue is prepared according to the following steps through the above-mentioned raw material formula in parts by weight:

[0031] 1) The rapeseed oil cake and natural rubber are stirred and pulverized by a stirring pulverizer to prepare a mixture for subsequent use;

[0032] 2) Pass pine resin and animal fat through a sealed container, heat and melt, and stir and mix. The heating temperature is 200-230° C., and the heating time is 90-120 minutes, and the mixed oil is prepared for use;

[0033] 3) Add the above-mentioned mixed oil into a sealed container, add the mixed material, and at the ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a badminton seat outer layer reinforcement adhesive formula and a production process thereof and relates to the technical field of production of badmintons. The badminton seat outer layer reinforcement adhesive formula comprises the following raw materials in parts by weight: 10-15 parts of resinous carbon, 10-15 parts of rap oil seedcake, 10-15 parts of animal fat, 6-10 parts of attapulgite powder, 6-10 parts of natural rubber and 8-12 parts of corn starch. Due to resinous carbon, aminal fat and rape oil seedcake included in the formula, the softness of the reinforce adhesive is effectively improved; due to attapulgite powder and corn starch included in the formula, the firmness and the compactness of the reinforcement adhesive are effectively improved; due to natural rubber included in the formula, the softness and the durability of the reinforcement adhesive are effectively improved; meanwhile, the main components of the raw materials of the formula are selected from biological materials, so that the formula is green and environmentally friendly; the pollution to the environment and the harm to the human health are reduced.

Description

Technical field: [0001] The invention relates to the technical field of badminton production, in particular to a formula of reinforcing glue for the outer layer of a badminton seat and a production process thereof. Background technique: [0002] In the badminton production process, the seat part of the produced shuttlecock needs to be reinforced twice to ensure the firmness between the ball seat and the feather and the impact resistance of the ball seat. Generally, it is sprayed or soaked in reinforcement glue. When the technical reinforcement glue is used to reinforce the badminton seat, it often causes the surface of the badminton seat to harden and crack during the hitting process, which cannot provide the proper protection and also cause certain damage to the racket. , when carrying out the outer layer reinforcement of badminton seat, need a kind of not only can increase firmness between ball seat and feather, but also can increase the softness, compactness and durabilit...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C09J193/04C09J191/00C09J107/00C09J103/02C09J11/04
CPCC09J193/04C08L2205/025C08L2205/035C09J11/04C09J191/00C08L91/00C08L7/00C08L3/02C08K3/346C08L93/04
Inventor 邵贤法沈在国翟建民丁百所倪友田
Owner 安徽太阳体育用品有限公司