Wax sealing method of wood floor
A wood floor and turpentine technology, applied to the surface coating liquid device, spray device, fat generation, etc., can solve the problems of increasing production costs, wax waste, splashing, etc., achieve uniform thickness of sealing wax, avoid secondary Pollution, the effect of solving friction noise
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A wax sealing method for wooden floors. The method is to pump turpentine into a conveying pipeline through a vacuum pump, and then start a nozzle connected to the conveying pipeline to spray the turpentine in a mist form to seal the grooves and tenons of the wooden floor; the nozzle sprays turpentine When the pressure is 0.9MPa; the flow rate of turpentine sprayed by the nozzle is 1.8g / s; this method realizes the input and output of the wooden floor by setting a conveying device under the nozzle, and the conveying device has a transmission speed of 20m / min; The recovery device is used to collect the turpentine oil that is not attached to the groove and tenon during the sealing wax. The turpentine oil is filtered and precipitated in the recovery device, and then recovered through the recovery pipeline to the oil storage container for reuse.
Embodiment 2
[0020] A wax sealing method for wooden floors. The method is to pump turpentine into a conveying pipeline through a vacuum pump, and then start a nozzle connected to the conveying pipeline to spray the turpentine in a mist form to seal the grooves and tenons of the wooden floor; the nozzle sprays turpentine When the pressure is 0.6MPa; the flow rate of the turpentine sprayed by the nozzle is 1g / s; this method realizes the input and output of the wooden floor by setting a conveying device under the nozzle, and the conveying device has a transmission speed of 10m / min; this method is recovered by setting The device is used to collect the turpentine oil that is not attached to the groove and tenon part during the sealing wax. The turpentine oil is filtered and precipitated in the recovery device, and then recovered through the recovery pipeline to the oil storage container for reuse.
Embodiment 3
[0022] A wax sealing method for wooden floors. The method is to pump turpentine into a conveying pipeline through a vacuum pump, and then start a nozzle connected to the conveying pipeline to spray the turpentine in a mist form to seal the grooves and tenons of the wooden floor; the nozzle sprays turpentine The pressure when the nozzle is 1.2MPa; the flow rate of the turpentine sprayed by the nozzle is 2g / s; this method realizes the input and output of the wooden floor by setting a conveying device under the nozzle, and the conveying device has a transmission speed of 30m / min; this method is recovered by setting The device is used to collect the turpentine oil that is not attached to the groove and tenon part during the sealing wax. The turpentine oil is filtered and precipitated in the recovery device, and then recovered through the recovery pipeline to the oil storage container for reuse.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com