Yarn sizing process for cotton-polyester blended fabric yarn
A cotton-polyester blending and yarn technology, which is applied in textiles, papermaking, plant fibers, wear-resistant fibers, etc., can solve the problems that performance needs to be improved, and achieve the effects of increased strength, yarn hairiness fit, and good wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The sizing process of cotton-polyester blended fabric yarn comprises the following steps:
[0026] 1) Put 1 to 2 parts by weight of glycerin rosin ester, 1.3 parts by weight of paraffin, 0.8 parts by weight of potassium persulfate, 2.2 parts by weight of hexyldecanol, and 15 parts by weight of phosphate starch into 25 parts by weight of deionized water in sequence, and stir evenly;
[0027] 2) drop into 0.9 parts by weight of sodium n-butyl naphthalene sulfonate, 1.2 parts by weight of isomeric fatty alcohol polyoxyethylene ether phosphate, 1.9 parts by weight of polyisobutylene, 1.7 parts by weight of polyoxyethylene stearic acid ester, and continue to stir, Until fully mixed evenly, a slurry is obtained;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of cotton-polyester blended fabric yarn comprises the following steps:
[0031] 1) Put 1 part by weight of glycerin rosin ester, 1.3 parts by weight of paraffin wax, 0.8 parts by weight of potassium persulfate, 2.2 parts by weight of hexyldecanol, and 15 parts by weight of starch phosphate into 25 parts by weight of deionized water in turn, and stir evenly;
[0032] 2) drop into 0.9 parts by weight of sodium n-butyl naphthalene sulfonate, 1.2 parts by weight of isomeric fatty alcohol polyoxyethylene ether phosphate, 1.9 parts by weight of polyisobutylene, 1.7 parts by weight of polyoxyethylene stearic acid ester, and continue to stir, Until fully mixed evenly, a slurry is obtained;
[0033] 3) Dip the yarn into the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of cotton-polyester blended fabric yarn comprises the following steps:
[0036] 1) Put 2 parts by weight of glycerin rosin ester, 1.3 parts by weight of paraffin wax, 0.8 parts by weight of potassium persulfate, 2.2 parts by weight of hexyldecanol, and 15 parts by weight of starch phosphate into 25 parts by weight of deionized water in sequence, and stir evenly;
[0037] 2) drop into 0.9 parts by weight of sodium n-butyl naphthalene sulfonate, 1.2 parts by weight of isomeric fatty alcohol polyoxyethylene ether phosphate, 1.9 parts by weight of polyisobutylene, 1.7 parts by weight of polyoxyethylene stearic acid ester, and continue to stir, Until fully mixed evenly, a slurry is obtained;
[0038] 3) Dip the yarn into the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com