[0025] The sizing process of cotton fabric yarn comprises the steps:
[0026] 1) 1 to 2 parts by weight of fatty acid triglycerides, 1.1 parts by weight of hydroxyethyl cellulose, 1.5 parts by weight of 2,6-di-tert-butyl p-cresol, 1.1 parts by weight of sodium tripolyphosphate, 14 parts by weight of corn The modified starch is dropped into 30 parts by weight of deionized water successively, and stirred evenly;
[0027] 2) Add 2.1 parts by weight of block polyoxyethylene-polyoxypropylene ether, 0.8 parts by weight of sodium alkyl sulfate, 1.2 parts by weight of phytic acid ester, and 0.9 parts by weight of fresh bark extract, and continue stirring until Mix well and make a slurry;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of cotton fabric yarn comprises the steps:
[0031] 1) 1 part by weight of fatty acid triglyceride, 1.1 parts by weight of hydroxyethyl cellulose, 1.5 parts by weight of 2,6-di-tert-butyl-p-cresol, 1.1 parts by weight of sodium tripolyphosphate, and 14 parts by weight of corn The starch is dropped into 30 parts by weight of deionized water successively, and stirred evenly;
[0032] 2) Add 2.1 parts by weight of block polyoxyethylene-polyoxypropylene ether, 0.8 parts by weight of sodium alkyl sulfate, 1.2 parts by weight of phytic acid ester, and 0.9 parts by weight of fresh bark extract, and continue stirring until Mix well and make a slurry;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of cotton fabric yarn comprises the steps:
[0036] 1) 2 parts by weight of fatty acid triglycerides, 1.1 parts by weight of hydroxyethyl cellulose, 1.5 parts by weight of 2,6-di-tert-butyl-p-cresol, 1.1 parts by weight of sodium tripolyphosphate, and 14 parts by weight of corn The starch is dropped into 30 parts by weight of deionized water successively, and stirred evenly;
[0037] 2) Add 2.1 parts by weight of block polyoxyethylene-polyoxypropylene ether, 0.8 parts by weight of sodium alkyl sulfate, 1.2 parts by weight of phytic acid ester, and 0.9 parts by weight of fresh bark extract, and continue stirring until Mix well and make a slurry;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com