A kind of steel slag hair slag method

A technology for steel slag and red slag, applied in the field of metallurgy, can solve the problems of high cost, large amount of slag water, poor stability of steel slag, etc., and achieve the effects of reducing the time of slag generation, prolonging the aging time, and accelerating the separation of slag and iron.

Active Publication Date: 2019-02-26
WUKUN STEEL
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Although the hot splashing method can effectively cool down the steel slag and is suitable for treating all steel slags, its disadvantages are that it occupies a large area during the treatment process, takes a long time for slag generation, and has a large amount of water for slag generation; the slag after treatment has high activity and poor stability. The effect of iron separation is not good, which is not conducive to magnetic separation, and the content of free calcium oxide in steel slag is high; the water content of steel slag is high, and the humidity of steel slag is high, so it is easy to stick to the belt and magnetic roller; the recovery rate of metal iron is low, the cost is high, and the effect is poor

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] Put the steel slag to be treated into the treatment pool and spray water. The steel slag to be treated is 8000 tons, and the water spray volume is 2440 m 3 , to control the red slag inside the steel slag when the water spraying is stopped, the temperature of the red slag is 300°C, and then use the temperature of the red slag to evaporate the steel slag on the surface, mix the red slag and the steel slag on the surface, and transport it to The slag-iron separation will be accelerated on the site of the magnetic separation section. The sprayed water is sprayed circulating water, that is, the sprayed water flows into the circulating pool, and is cooled and reused.

[0018] Adopt the steel slag hair slag method of embodiment 1 of the present invention, the free calcium oxide of sampling test result is 9.16%, far lower than 15.66% of conventionally used hot pouring method by 6.5%. Adopt the steel slag hair slag method of embodiment 1 to process 305,905 tons of steel slag in...

Embodiment 2

[0020] Put the steel slag to be treated into the treatment pool and spray water. The steel slag to be treated is 8500 tons, and the water spray volume is 2400 m 3 , to control the inside of the steel slag to have red slag when water spraying is stopped, the temperature of the red slag is 350°C, then use the temperature of the red slag to evaporate the steel slag on the surface, mix the red slag and the steel slag on the surface, and transport to The slag-iron separation will be accelerated on the site of the magnetic separation section. The sprayed water is sprayed circulating water, that is, the sprayed water flows into the circulating pool, and is cooled and reused.

[0021] Practice has proved that the process modification scheme is simple and easy to implement without investment.

Embodiment 3

[0023] Put the steel slag to be treated into the treatment pool and spray water. The steel slag to be treated is 9000 tons, and the water spray volume is 2500m 3 , when the water spraying is stopped, there is red slag inside the steel slag, the temperature of the red slag is 400°C, then the steel slag on the surface is evaporated to dryness by using the temperature of the red slag, the red slag is mixed with the steel slag on the surface, and transported to The slag-iron separation will be accelerated on the site of the magnetic separation section. The sprayed water is sprayed circulating water, that is, the sprayed water flows into the circulating pool, and is cooled and reused.

[0024] Practice has proved that the process modification scheme is simple and easy to implement without investment.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a slagging method for slag. The slagging method for slag comprises the steps of: stopping spraying water when the inner side of the slag is red, shortening the slagging time and controlling the slagging water quantity; and evaporating the slag on the surface by virtue of the temperature of the red slag, blending the high-temperature red slag with the slag and conveying the mixture to a magnetic separation work section site to be continuously cured to prolong the curing time and accelerate separation of the slag and iron, wherein magnetic separation is further facilitated and free calcium oxide in the slag is further exerted to the maximum extent. Meanwhile, the water content of the slag is reduced, the hidden danger that the slag which is high in humidity is sticky to equipment such as a belt and a magnetic separation barrel is eliminated, the metal iron recovery rate is improved, and the purposes of directly improving the output of washed grained iron and washed ball-milled waste slag steel, decreasing the cost and increasing the benefit are achieved.

Description

technical field [0001] The invention belongs to the technical field of metallurgy, and in particular relates to a steel slag generating method. Background technique [0002] Steel slag is a major companion in the production process of iron and steel enterprises. As a derivative of the steelmaking process, its annual output is also increasing with the increase in steel production. Steel slag is a potential resource that must be recovered and utilized. Steel slag is a by-product of steelmaking, and its output is generally 12% to 20% of crude steel output. Storing steel slag not only wastes a lot of land, but also poses a serious threat to the environment. Improve the steel slag processing capacity and technical level, and accelerate The comprehensive utilization of steel slag is imminent. Selecting and applying advanced and effective steel slag treatment process and resource utilization new technology to achieve effective separation of slag and iron and comprehensive utiliza...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): C21B3/06
CPCC21B3/06Y02P10/20Y02W30/50
Inventor 赵杰
Owner WUKUN STEEL
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products