[0028] This example is used to illustrate the oil-based foaming method of the present invention.
[0029] (1) disodium lauryl sulfosuccinate (LT-60), cocamidopropyl betaine (CAB-35), ethylene glycol butyl ether, isopropanol, and water in a mass ratio of 50:15: Mix at 10:5:20, take 1 gram of the prepared mixture in 100ml of palm oil, add 2 grams of ethylene-propylene-diene copolymer (EPDM) to fully dissolve to form foamable palm oil.
[0030] (2) Adopt sand core drying nitrogen bubbling method, install sand core bubbler at the bottom of the measuring cylinder, pour the foamable palm oil into the measuring cylinder, start bubbling, the foam volume increases, when the upper foam bursting speed and When the foam generation speed in the lower part is equal, the foam height tends to be stable. At this time, record the foam height as the foam volume (initial volume), stop bubbling, and record the time when the foam volume is reduced to half of the initial volume, which is recorded as...
Embodiment 2
[0032] This example is used to illustrate the oil-based foaming method of the present invention.
[0033](1) Disodium lauryl ether sulfosuccinate monoester (MES-30), lauryl amidopropyl betaine (LAB-30), butyl glycol ether, isopropanol, and water in a mass ratio of 40:20 : 10:6:20 mixing, take 1.5 grams of prepared foaming agent in 100ml palm oil, add 1 gram of ethylene propylene copolymer (OCP) to fully dissolve to form foamable palm oil.
[0034] (2) Adopt sand core drying nitrogen bubbling method, install sand core bubbler at the bottom of the measuring cylinder, pour the foamable palm oil into the measuring cylinder, start bubbling, the foam volume increases, when the upper foam bursting speed and When the foam generation speed in the lower part is equal, the foam height tends to be stable. At this time, record the foam height as the foam volume (initial volume), stop bubbling, and record the time when the foam volume is reduced to half of the initial volume, which is recor...
Embodiment 3
[0036] This example is used to illustrate the oil-based foaming method of the present invention.
[0037] (1) Dioctyl sodium sulfosuccinate (penetrant T), dodecyl dimethyl betaine (BS-12), butyl glycol ether, isopropanol, and water are mixed in a mass ratio of 45:10 :15:5:15 mixing, take 1 gram of the prepared mixture in 100ml palm oil, add 2 grams of hydrogenated styrene diene copolymer (HSD) to fully dissolve to form foamable palm oil.
[0038] (2) Adopt sand core drying nitrogen bubbling method, install sand core bubbler at the bottom of the measuring cylinder, pour the foamable palm oil into the measuring cylinder, start bubbling, the foam volume increases, when the upper foam bursting speed and When the foam generation speed in the lower part is equal, the foam height tends to be stable. At this time, record the foam height as the foam volume (initial volume), stop bubbling, and record the time when the foam volume is reduced to half of the initial volume, which is record...