A carvacrol, nanoemulsion technology, applied in the directions of botanical equipment and methods, chemicals for biological control, and repellents, etc., can solve problems affecting bioavailability and scope of application, poor stability, easy oxidation, etc. problem, to achieve the effect of improving bioavailability, strong stability and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] This example is an example of preparation and property testing of the nanoemulsion composition of the present invention.
[0029] 1. Preparation of carvacrol nanoemulsion composition:
[0030] 0.50 g of carvacrol and 1.25 g of corn oil were weighed and mixed to form an oil phase, then 1.75 g of Tween-80 and 5.00 g of propylene glycol were added to the oil phase and stirred to obtain a mixed oil phase;
[0031] Add 50.00 g of acidic electrolyzed water and 41.50 g of deionized water to the mixed oil phase obtained in the above steps, and stir to obtain a mixed solution;
[0032] The mixed solution was placed in an ultrasonic cell disruptor for ultrasonic treatment, the ultrasonic power was 1000 W, the ultrasonic frequency was 20 kHz, and the ultrasonic time was 10 min to obtain carvacrol nanoemulsion.
[0033] The acidic electrolyzed water used in the above-mentioned preparation steps can be an aqueous solution formed by electrolyzing 18% (w / v) sodium chloride by an elec...
Embodiment 2
[0042] This example is an example of preparation and property testing of the nanoemulsion composition of the present invention.
[0043] 1. Preparation of carvacrol nanoemulsion composition:
[0044] 0.50 g of carvacrol and 2.00 g of corn oil were weighed and mixed to form an oil phase, then 2.00 g of Tween-80 and 6.00 g of propylene glycol were added to the oil phase and stirred to obtain a mixed oil phase;
[0045] Add 50.00 g of acidic electrolyzed water and 39.50 g of deionized water to the mixed oil phase obtained in the above steps, and stir to obtain a mixed solution;
[0046] The mixed solution was placed in an ultrasonic cell disruptor for ultrasonic treatment, the ultrasonic power was 1000 W, the ultrasonic frequency was 20 kHz, and the ultrasonic time was 10 min to obtain carvacrol nanoemulsion.