Strengthening technology for improving service characteristic of wicker products
A kind of weaving and characteristic technology, applied in the field of willow weaving, can solve the problems of cracking, weak effect, weakening of branch hardness, etc., and achieve the effect of increasing service life and improving mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] A strengthening process for improving the use characteristics of willow products, comprising the following steps:
[0027] (1) Vacuum exhaust treatment:
[0028] Put the willow weaving after weaving into the pressure treatment tank, then vacuumize the pressure treatment tank, and treat it for 40 minutes for later use;
[0029] (2) Modified liquid treatment:
[0030] After the vacuum exhaust treatment of the wickerwork is completed, keep the vacuum pump in the pressure treatment tank turned on, and then inject the modified liquid into the pressure treated tank. When the modified liquid is completely immersed in the wickerwork and the pressure tank is full, turn off the vacuum pump, and Pressurize the pressure treatment tank, increase the pressure to 1.5MPa, and keep the pressure for 25 minutes; the modified liquid is composed of the following parts by weight: 90 parts of silica sol, 5 parts of titanate coupling agent, 2 parts of hydroxy silicone oil, 1 part of Chinese ...
Embodiment 2
[0043] A strengthening process for improving the use characteristics of willow products, comprising the following steps:
[0044] (1) Vacuum exhaust treatment:
[0045] Put the wickerwork after weaving into the pressure treatment tank, then vacuumize the pressure treatment tank, and treat it for 43 minutes for later use;
[0046] (2) Modified liquid treatment:
[0047] After the vacuum exhaust treatment of the wickerwork is completed, keep the vacuum pump in the pressure treatment tank turned on, and then inject the modified liquid into the pressure treated tank. When the modified liquid is completely immersed in the wickerwork and the pressure tank is full, turn off the vacuum pump, and Pressurize the pressure treatment tank to increase the pressure to 1.8 MPa, and keep the pressure for 28 minutes; the modified liquid is composed of the following parts by weight: 95 parts of silica sol, 7 parts of titanate coupling agent, 4 parts of hydroxyl silicone oil, 2 parts of Chinese...
Embodiment 3
[0060] A strengthening process for improving the use characteristics of willow products, comprising the following steps:
[0061] (1) Vacuum exhaust treatment:
[0062] Put the finished wickerwork into the pressure treatment tank, then vacuumize the pressure treatment tank, and treat it for 45 minutes for later use;
[0063] (2) Modified liquid treatment:
[0064] After the vacuum exhaust treatment of the wickerwork is completed, keep the vacuum pump in the pressure treatment tank turned on, and then inject the modified liquid into the pressure treated tank. When the modified liquid is completely immersed in the wickerwork and the pressure tank is full, turn off the vacuum pump, and Pressurize the pressure treatment tank, increase the pressure to 2MPa, and keep the pressure for 30 minutes; the modified liquid is composed of the following parts by weight: 100 parts of silica sol, 8 parts of titanate coupling agent, 5 parts 1 part of hydroxy silicone oil, 3 parts of Chinese me...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com