Dolomite mineralization method

A dolomite and soluble technology, which is applied in the field of dolomite mineralization, can solve the problems that the surface properties are very different from those of dolomite, the surface and interface properties such as wettability, adsorption, and polarity are far apart, and restrict development.

Inactive Publication Date: 2017-11-07
QINGYANG COUNTY YONGCHENG CALCIUM IND
View PDF0 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The study of dolomite reservoirs not only faces the difficulty of artificial synthesis of dolomite, but also the artificial simulation of dolomite porous media
At present, some materials are commonly used in the academic circles to replace dolomite reservoirs, such as porous sandstone, porous 3D printing models, etc., but due to the different chemical compositions of materials, the surface properties are very different from those of dolomite. The surface and interface properties such as wettability, adsorption and polarity are very different, which restricts the development of research in this field.
[0004] At present, there is no method for uniform dolomite mineralization on the inner surface of porous media containing internal spaces such as pores, cracks, and cavities. Therefore, it is necessary to provide a mineralization treatment method to achieve dolomite mineralization on the inner surface of porous media materials.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0016] A dolomite mineralization method, the method includes the following steps:

[0017] (1) Completely immerse the porous media material in the dolomite mineralized liquid, and apply a vacuum to keep the system in a vacuum state;

[0018] (2) After vacuuming, keep it under this pressure for 4 hours, then return to normal pressure and keep it for 15 hours, so that the above internal space is filled with fully saturated CaCO 3 Mineralized liquid.

[0019] (3) Increase the temperature or pressure in the container from room temperature and normal pressure to 800°C and 6MPa respectively, and keep it for 36 hours to complete the mineralization of dolomite on the inner surface of the porous media material, and then return to normal temperature and pressure.

[0020] Further, the dolomite mineralization liquid is an aqueous solution of a soluble calcium salt, a soluble magnesium salt and a slow release agent of carbonate, and the volume concentration of the above soluble calcium salt, a sol...

Embodiment 2

[0024] A dolomite mineralization method, the method includes the following steps:

[0025] (1) Completely immerse the porous media material in the dolomite mineralized liquid, and apply a vacuum to keep the system in a vacuum state;

[0026] (2) After vacuuming, keep it under this pressure for 2 hours, then return to normal pressure and keep it for 10 hours, so that the above internal space is filled with fully saturated CaCO 3 Mineralized liquid.

[0027] (3) Increase the temperature or pressure in the container from room temperature and normal pressure to 600°C and 5MPa, and keep it for 20 hours to complete dolomite mineralization on the inner surface of the porous media material, and then return to normal temperature and pressure.

[0028] Further, the dolomite mineralization liquid is an aqueous solution of a soluble calcium salt, a soluble magnesium salt and a slow release agent of carbonate, and the volume concentration of the above soluble calcium salt, a soluble magnesium salt ...

Embodiment 3

[0032] A dolomite mineralization method, the method includes the following steps:

[0033] (1) Completely immerse the porous media material in the dolomite mineralized liquid, and apply a vacuum to keep the system in a vacuum state;

[0034] (2) After vacuuming, keep it under this pressure for 5 hours, then return to normal pressure and keep it for 20 hours, so that the above internal space is filled with fully saturated CaCO 3 Mineralized liquid.

[0035] (3) Increase the temperature or pressure in the container from room temperature and normal pressure to 1200°C and 10MPa respectively, and keep it for 48 hours to complete the mineralization of dolomite on the inner surface of the porous media material, and then return to normal temperature and pressure.

[0036] Further, the dolomite mineralization liquid is an aqueous solution of a soluble calcium salt, a soluble magnesium salt and a slow release agent of carbonate, and the volume concentration of the above soluble calcium salt, a s...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
Pore diameteraaaaaaaaaa
Pore diameteraaaaaaaaaa
Pore diameteraaaaaaaaaa
Login to View More

Abstract

The invention provides a dolomite mineralization method, comprising the steps of: (1) fully immersing the porous medium material in the dolomite mineralization liquid, and vacuumizing the system to maintain a vacuum state; Keep it under pressure for 2-5 hours, then return to normal pressure and keep it for 10-20 hours, so that the above-mentioned internal space is filled with fully saturated CaCO3 mineralized liquid. (3) The temperature or pressure in the container is raised from room temperature and normal pressure to 600-1200°C, 5-10MPa, and kept for 20-48 hours to complete the mineralization of dolomite on the inner surface of the porous media material, and then return to Temperature and pressure. This method can realize dolomite mineralization in difficult-to-reach positions such as the inner surface of porous media; it can make dolomite mineralization form a thinner dolomite film, which is higher than the existing co-precipitation or ion exchange methods. Calcite; can realize the simulation of dolomite reservoir core in the oil and gas field.

Description

Technical field [0001] The invention relates to the field of dolomite processing, in particular to a dolomite mineralization method. Background technique [0002] Dolomite is a trigonal system of CaMg (CO 3 ) 2 , Is one of the most common carbonate minerals and one of the most difficult to simulate synthetic minerals. There was a large number of dolomite in the marine strata of the Paleozoic. According to research, its formation may be related to the slow action of sulfate-reducing bacteria. However, it is difficult to synthesize dolomite under low-temperature seawater conditions in modern laboratories. The Dolomite Problem". [0003] Dolomite formation is one of the main oil reservoirs in the world, and it has the common characteristics of porous media. The study of dolomite reservoirs not only faces the difficulty of artificial synthesis of dolomite, but also the artificial simulation of dolomite porous media. At present, some materials are commonly used in academia to replace...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine