Unlock instant, AI-driven research and patent intelligence for your innovation.

A kind of grinding additive for X-ray fluorescence spectrometry analysis sample preparation and using method

A fluorescence spectroscopy, additive technology, applied in fluorescence/phosphorescence, material analysis by optical means, analysis of materials, etc., can solve problems such as the inability to achieve the required particle size

Active Publication Date: 2021-02-23
ANGANG STEEL CO LTD
View PDF14 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] With the increasing application of X-ray fluorescence spectrometer in the field of inorganic chemical analysis, the requirements for sample preparation technology before sample analysis are getting higher and higher. In order to ensure the accuracy of analysis results, the particle size of sample preparation is very strict, but some The physical properties of some flux and pellet samples make them unable to reach the required particle size

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0020] 40 g of pellet samples were prepared.

[0021] Preparation of auxiliary grinding additive: ethanol (95% analytically pure) 30ml

[0022] Triethanolamine (analytical purity>95%) 20ml

[0023] Sodium stearate (analytical grade) 4g

[0024] The preparation method of the grinding aid additive: make a mixed solution of ethanol and triethanolamine according to the above ratio, mix well, add sodium stearate and mix thoroughly for use.

[0025] 2 ml of the above-mentioned additives were added to 40 g of the sample. The broken particle size finally reaches less than 0.050mm.

Embodiment 2

[0027] Prepare 20 g of dolomite samples.

[0028] Preparation of auxiliary grinding additive: ethanol (95% analytically pure) 30ml

[0029] Triethanolamine (analytical purity>95%) 30ml

[0030] Sodium stearate (analytical grade) 5g

[0031] The preparation method of the grinding aid additive: make a mixed solution of ethanol and triethanolamine according to the above ratio, mix well, add sodium stearate and mix thoroughly for use.

[0032] 1 ml of the above-mentioned additives was added to 20 g of the sample. The broken particle size finally reaches less than 0.050mm.

Embodiment 3

[0034] Prepare 40 g of limestone samples.

[0035] Preparation of auxiliary grinding additive: ethanol (95% analytically pure) 40ml

[0036] Triethanolamine (analytical purity>95%) 30ml

[0037] Sodium stearate (analytical grade) 7g

[0038] The preparation method of the grinding aid additive: make a mixed solution of ethanol and triethanolamine according to the above ratio, mix well, add sodium stearate and mix thoroughly for use.

[0039] 2 ml of the above-mentioned additives were added to 40 g of the sample. The broken particle size finally reaches less than 0.050mm.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
particle sizeaaaaaaaaaa
Login to View More

Abstract

The invention relates to an X-ray fluorescence spectrometry analysis of a grinding additive for sample preparation and a method of use. The additive includes ethanol (95% analytical purity), triethanolamine (analytic purity>95%), sodium stearate (analytic purity), The volume ratio of ethanol and triethanolamine is (1~2):1; add 3~5 grams of sodium stearate to every 50 ml of ethanol and triethanolamine mixture. Add this additive during the sample preparation process, so that the particle size effect cannot be produced between the fine particles during the grinding process of the sample. Eliminate the adsorption force between the sample particles, increase the tension between the sample particles, so that the sample cannot adhere to a ball or cake during the grinding process, and hinder the further crushing of the sample particle size. Make the broken particle size of the sample finally reach less than 0.050mm.

Description

technical field [0001] The invention relates to a grinding aid additive for X-ray fluorescence spectrometry analysis sample preparation and a use method. Background technique [0002] With the increasing application of X-ray fluorescence spectrometer in the field of inorganic chemical analysis, the requirements for sample preparation technology before sample analysis are getting higher and higher. In order to ensure the accuracy of analysis results, the particle size of sample preparation is very strict, but some The physical properties of some flux and pellet samples make them unable to reach the required particle size. Contents of the invention [0003] The technical problem to be solved by the present invention is to provide a grinding aid for X-ray fluorescence spectrometry analysis sample preparation, so that the particle size of the sample can overcome the shortcomings of its own physical properties and reach the particle size required by X-ray fluorescence spectrome...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): G01N21/64G01N1/28
CPCG01N1/286G01N21/64G01N2001/2866G01N2021/6417
Inventor 王丽晖黄宗仁高巍张道光李奎